Tsarin sinadarai
SiO₂ 79.62%, K₂O 10.53%, CaO 2.8%, P₂O₅ 1.61%, MnO 0.71%, MgO 0.89%, Fe₂O₃ 0.26%, Al₂O₃ 0.27%, Na₂O 0.35%, LOI 2.92%
Ana kuma kiransa
藁灰, わら灰, warabai, Rice straw ash
Kayan aiki masu kama
Synthetic Rice-Straw Ash (合成藁灰)
Tushe
Guzmán A., Delvasto S., Sánchez E., 'Valorization of rice straw waste: an alternative ceramic raw material', Cerâmica 61 (357), 2015, Table II, process D (XRF) (2015)

Na tarihi: maginan tukwane suna yin nasu ta hanyar ƙona karan shinkafa, kuma ba a sayar da shi a matsayin daidaitaccen kaya. Wannan samfuri ɗaya ne, na karan shinkafar Colombia da aka ƙona a murhun waje sannan aka dumama shi zuwa 800 °C na awa 2, ba a wanke ba. Tokar kara tana bambanta da karan, ƙasa da ƙonawar: a cikin wannan binciken, ƙonawa mai zafi ta ba da silica mai yawa da ƙarancin potash, kuma tokar karan shinkafa ta Digitalfire tana da SiO₂ 77.26% amma K₂O 3.29% kawai. Ana ƙirga chlorine ɗinsa na 0.59% da sulfur na 1.74% a nan a matsayin abin da ya ɓace a gasa.

Binciken oxide da UMF

Glazecalc yana da binciken Rice-Straw Ash (藁灰) a matsayin kashi bisa nauyi na ɗanyen kayan. Gudummawar UMF ita ce mole na kowane oxide a cikin adadin Rice-Straw Ash (藁灰) da ke ɗauke da mole 1.0 na flux, kuma haka Glazecalc ke ƙara shi cikin UMF (unity molecular formula) na tsarin glaze.

Oxide a cikin Rice-Straw Ash (藁灰)
Oxide Kashi bisa nauyi % Gudummawar UMF
SiO₂79.626.644
K₂O10.530.560
CaO2.80.250
P₂O₅1.610.057
MnO0.710.050
MgO0.890.111
Fe₂O₃0.260.008
Al₂O₃0.270.013
Na₂O0.350.028
Nauyin daidai (equivalent weight)
501.36
Nauyi bayan gasa
486.72
LOI (raguwar nauyi a wuta)
2.92%

Nauyin daidai shi ne giram na Rice-Straw Ash (藁灰) da ke ɗauke da mole 1.0 na flux. Nauyi bayan gasa shi ne abin da ya rage daga wannan bayan gasa.

Haɗari da tsaro

Haɗari: Yana ɗauke da crystalline silica, kuma tokar da ba a wanke ba tana ƙona fata (caustic) idan ta jiƙe; ku sa safar hannu kuma ku guji shaƙar ƙurar.

Glazecalc yana nuna kalmomin haɗari kamar yadda bayanin laburaren ya ba da su. Wannan ba cikakken kimanta haɗari ba ne, don haka ku karanta takardar bayanan aminci daga mai sayar muku. Kafin ku taɓa kowane kayan glaze, ku karanta Haɗawa cikin aminci da iska mai kyau da Kada ka sa wa iyalinka guba.

Yi amfani da shi a tsarin glaze

Ƙara Rice-Straw Ash (藁灰) cikin tsarin glaze a kalkuletan Glazecalc don ganin abin da yake yi wa UMF na glaze.

Buɗe kalkuletan tsarin glazeDuk kayan aiki na asali

Buɗe asusu kyauta