Mene ne shi

Nau’i
Flux (masu narkarwa)
Tsarin sinadarai
SiO₂ 81.46%, Al₂O₃ 6.52%, Fe₂O₃ 0.14%, CaO 2.83%, MgO 1.1%, Na₂O 1.7%, K₂O 1.65%, LOI 4.6%
Ana kuma kiransa
合成藁灰, 合成ワラ灰, 合成わら灰, gōsei warabai
Ana sayar da shi a
JP
Tushe
佐賀県陶磁器原料株式会社 (Arita): 釉薬原料の化学分析表, the supplier's typical analysis of what it sells (undated; read 2026-11-04). Second analysis: 吉田博和ほか「笠間焼の新素地・新釉薬の開発」, 茨城県工業技術センター研究報告 43 (2014), 表6

Nazari na yau da kullum daga mai sayarwa ɗaya a Arita: kwatanta shi da na mai sayar muku. Madadin da aka ƙera (synthetic) na 藁灰, tokar karan shinkafa da ke sa glaze na Japan su yi fari kamar madara; galibi silica ne. Adadin mai sayarwar ya kai 97.1%, don haka 2.9% da suka bari ana ƙirga shi a nan a matsayin abin da ya ɓace a gasa, tare da LOI ɗinsa na 1.7%. Nazarin 2014 na cibiyar fasahar masana'antu ta Ibaraki na wani 合成藁灰 ya kusan zama ɗaya: SiO₂ 80.6%, Al₂O₃ 7.7%, CaO 2.9%, LOI 1.5%.

Binciken oxide da UMF

Glazecalc yana da binciken Synthetic Rice-Straw Ash (合成藁灰) a matsayin kashi bisa nauyi na ɗanyen kayan. Gudummawar UMF ita ce mole na kowane oxide a cikin adadin Synthetic Rice-Straw Ash (合成藁灰) da ke ɗauke da mole 1.0 na flux, kuma haka Glazecalc ke ƙara shi cikin UMF (unity molecular formula) na tsarin glaze.

Oxide a cikin Synthetic Rice-Straw Ash (合成藁灰)
Oxide Kashi bisa nauyi % Gudummawar UMF
SiO₂81.4611.049
Al₂O₃6.520.521
Fe₂O₃0.140.007
CaO2.830.411
MgO1.10.222
Na₂O1.70.224
K₂O1.650.143
Nauyin daidai (equivalent weight)
814.97
Nauyi bayan gasa
777.48
LOI (raguwar nauyi a wuta)
4.6%

Nauyin daidai shi ne giram na Synthetic Rice-Straw Ash (合成藁灰) da ke ɗauke da mole 1.0 na flux. Nauyi bayan gasa shi ne abin da ya rage daga wannan bayan gasa.

Haɗari da tsaro

Haɗari: Yana ƙunshe da crystalline silica; ku guji shaƙar ƙurar.

Glazecalc yana nuna kalmomin haɗari kamar yadda bayanin laburaren ya ba da su. Wannan ba cikakken kimanta haɗari ba ne, don haka ku karanta takardar bayanan aminci daga mai sayar muku. Kafin ku taɓa kowane kayan glaze, ku karanta Haɗawa cikin aminci da iska mai kyau da Kada ka sa wa iyalinka guba.

Yi amfani da shi a tsarin glaze

Ƙara Synthetic Rice-Straw Ash (合成藁灰) cikin tsarin glaze a kalkuletan Glazecalc don ganin abin da yake yi wa UMF na glaze.

Buɗe kalkuletan tsarin glazeDuk kayan aiki na asali

Buɗe asusu kyauta