Synthetic Rice-Straw Ash (合成藁灰)
Okokwakha okujwayelekile kumtapo we-Glazecalc: ukuhlaziywa kwako kwe-oxide, isabelo se-unity nezingozi.
Kuyini
- Uhlobo
- Ama-flux
- I-formula
- SiO₂ 81.46%, Al₂O₃ 6.52%, Fe₂O₃ 0.14%, CaO 2.83%, MgO 1.1%, Na₂O 1.7%, K₂O 1.65%, LOI 4.6%
- Kubizwa nangokuthi
- 合成藁灰, 合成ワラ灰, 合成わら灰, gōsei warabai
- Kuthengiswa e
- JP
- Umthombo
- 佐賀県陶磁器原料株式会社 (Arita): 釉薬原料の化学分析表, the supplier's typical analysis of what it sells (undated; read 2026-11-04). Second analysis: 吉田博和ほか「笠間焼の新素地・新釉薬の開発」, 茨城県工業技術センター研究報告 43 (2014), 表6
Ukuhlaziywa okujwayelekile okuvela kumphakeli oyedwa e-Arita: kuqhathanise nokomphakeli wakho. Okufakwa esikhundleni okwenziwe (synthetic) kwe-藁灰, umlotha wezinhlanga zelayisi owenza ama-glaze aseJapan abe nombala wobisi; ikakhulukazi uyi-silica. Izibalo zomphakeli zihlangana zibe ngu-97.1%, ngakho u-2.9% abawushiyayo ubalwa lapha njengolahleka ekushiseni, ne-LOI yawo engu-1.7%. Ukuhlaziywa kwango-2014 kwesikhungo sobuchwepheshe bezimboni sase-Ibaraki kwenye i-合成藁灰 kwakucishe kufane: SiO₂ 80.6%, Al₂O₃ 7.7%, CaO 2.9%, LOI 1.5%.
Ukuhlaziywa kwe-oxide ne-unity formula
I-Glazecalc inokuhlaziywa kwe-Synthetic Rice-Straw Ash (合成藁灰) njengephesenti lesisindo sokokwakha okuluhlaza. Isabelo se-unity singama-mole e-oxide ngayinye enanini le-Synthetic Rice-Straw Ash (合成藁灰) eliqukethe i-mole engu-1.0 ye-flux, okuyindlela i-Glazecalc eyengeza ngayo ku-unity formula yeresiphi.
| I-oxide | Isisindo % | Isabelo se-unity |
|---|---|---|
| SiO₂ | 81.46 | 11.049 |
| Al₂O₃ | 6.52 | 0.521 |
| Fe₂O₃ | 0.14 | 0.007 |
| CaO | 2.83 | 0.411 |
| MgO | 1.1 | 0.222 |
| Na₂O | 1.7 | 0.224 |
| K₂O | 1.65 | 0.143 |
- Isisindo esilinganayo
- 814.97
- Isisindo esishisiwe
- 777.48
- I-loss on ignition
- 4.6%
Isisindo esilinganayo singamagremu e-Synthetic Rice-Straw Ash (合成藁灰) aqukethe i-mole engu-1.0 ye-flux. Isisindo esishisiwe yilokho okusalayo kulokho ngemva kokushisa.
Izingozi nokuphepha
Izingozi: Kuqukethe i-silica eyikristalu; gwema ukuhogela uthuli.
Kusebenzise eresiphini
Engeza i-Synthetic Rice-Straw Ash (合成藁灰) eresiphini ku-calculator ye-Glazecalc ukuze ubone ukuthi yenzani ku-unity formula ye-glaze.