Ihe ọ bụ

Ụdị
Flux
Formula
SiO₂ 81.46%, Al₂O₃ 6.52%, Fe₂O₃ 0.14%, CaO 2.83%, MgO 1.1%, Na₂O 1.7%, K₂O 1.65%, LOI 4.6%
A na-akpọkwa ya
合成藁灰, 合成ワラ灰, 合成わら灰, gōsei warabai
A na-ere ya na
JP
Ebe o si
佐賀県陶磁器原料株式会社 (Arita): 釉薬原料の化学分析表, the supplier's typical analysis of what it sells (undated; read 2026-11-04). Second analysis: 吉田博和ほか「笠間焼の新素地・新釉薬の開発」, 茨城県工業技術センター研究報告 43 (2014), 表6

Nyocha a na-ahụkarị site n'aka otu onye na-ere ahịa na Arita: tụnyere ya na nke onye na-ere gị. Ihe nnọchi e mepụtara (synthetic) maka 藁灰, ntụ ahịhịa osikapa na-eme ka glaze Japan dị ka mmiri ara ehi; ọ bụ silica ka ukwuu. Ọnụ ọgụgụ onye na-ere ahịa ruru 97.1%, ya mere a na-agụ 2.9% ha hapụrụ ebe a dịka ihe furu efu n'ọkụ, ya na LOI ya nke 1.7%. Nyocha 2014 nke ụlọ ọrụ teknụzụ ụlọ ọrụ Ibaraki mere na 合成藁灰 ọzọ fọrọ nke nta ka ọ dị otu: SiO₂ 80.6%, Al₂O₃ 7.7%, CaO 2.9%, LOI 1.5%.

Nyocha oxide na unity formula

Glazecalc nwere nyocha Synthetic Rice-Straw Ash (合成藁灰) dịka pasent ịdị arọ nke ihe ahụ a na-agbabeghị ọkụ. Ntinye unity bụ moles nke oxide ọ bụla n'ọnụ ọgụgụ Synthetic Rice-Straw Ash (合成藁灰) nke nwere 1.0 mole nke flux; otu a ka Glazecalc si agbakwunye ya n'unity formula nke usoro.

Oxide dị na Synthetic Rice-Straw Ash (合成藁灰)
Oxide Ịdị arọ % Ntinye unity
SiO₂81.4611.049
Al₂O₃6.520.521
Fe₂O₃0.140.007
CaO2.830.411
MgO1.10.222
Na₂O1.70.224
K₂O1.650.143
Ịdị arọ nhata (equivalent weight)
814.97
Ịdị arọ mgbe a gbara ọkụ
777.48
Loss on ignition (LOI)
4.6%

Ịdị arọ nhata bụ grams nke Synthetic Rice-Straw Ash (合成藁灰) nke nwere 1.0 mole nke flux. Ịdị arọ mgbe a gbara ọkụ bụ ihe fọdụrụ na ya mgbe a gbachara ọkụ.

Ihe ize ndụ na nchekwa

Ihe ize ndụ: O nwere crystalline silica; zere iku uzuzu ya.

Glazecalc na-egosi okwu ihe ize ndụ dịka ndekọ ọbá akwụkwọ si dee ya. Ọ bụghị nyocha ihe ize ndụ zuru ezu, ya mere gụọ mpempe data nchekwa site n'aka onye na-ere gị ya. Tupu i metụ ihe glaze ọ bụla, gụọ Ịgwakọta n'enweghị ihe ize ndụ na ikuku dị ọcha na Enyela ezinụlọ gị nsí.

Jiri ya n'usoro

Tinye Synthetic Rice-Straw Ash (合成藁灰) n'usoro na Glazecalc calculator ka ị hụ ihe ọ na-eme unity formula nke glaze.

Mepee calculator usoroIhe niile a na-ejikarị

Mepụta akaụntụ n'efu