Mepụta akaụntụ n'efu ma ọ bụ banye iji debe ndụmọdụ nke gị.

Ndụmọdụ izugbe

  • Nwee usoro

    Nwee usoro n'otu i si arụ ọrụ gị. Dee ihe ị na-eme n'otu ụzọ mgbe niile, debekwa ndekọ ndị ahụ ọnụ. Ịzụlite ezigbo usoro maka itinye glaze na ịgwakọta ga-ebelata oge, mgbalị na mmejọ.

    Mkpado: usoro, ụzọ ọrụ, ndekọ
  • Specific gravity

    Ịgwakọta glaze gị ka ọ nwee otu ịdị arọ (density), ma ọ bụ specific gravity, mgbe niile ga-enyere gị aka nke ukwuu iru ihe mgbaru ọsọ gị. Dee ihe ị tụrụ (density ma ọ bụ specific gravity) ka i wee soro mmetụta mgbanwe dị iche iche.

    Mkpado: specific gravity, density, ịgwakọta
  • Ịgba bisque (ọkụ mbụ)

    Hiwe usoro ịgba bisque nke na-adịgide otu, ma maka cone ma maka ọsọ. Nke a ga-edobe ntọala ka ite gị nwee otu ọnụego ha si aṅụ glaze. Ibelata mgbanwe n'akụkụ a nke ọrụ ga-enyere aka n'inyocha na ijikwa glaze.

    Mkpado: ịgba bisque, bisque firing, bisc firing, bisque-firing, nkwadebe, ụzọ ọrụ
  • Azachala ala

    Azachala ala studio ma ọ bụ ụlọ glaze mgbe ọ bụla.Ụzọ kacha mma iji hichaa ala bụ iji mop dị mmiri mmiri. Sponge ndị ọrụ ụlọ (contractor sponge) ga-arụ ọrụ nke ọma n'ebe nwere oyi akwa siri ike. Uzuzu bụ ihe a na-apụghị izere mgbe a na-arụ ọrụ na ụrọ na ihe glaze, ịza ala na-ebulikwa ya n'ikuku.

    Mkpado: uzuzu, ihe ize ndụ, idebe ụlọ ọcha
  • Akara na-adịgide adịgide

    Tinye akara na-adịgide adịgide n'ihe glaze na n'arịa glaze. Nke a dị mkpa okpukpu abụọ maka ihe nwere ihe ize ndụ, ndị a na-ahụkarị n'ihe na-enye glaze agba, ya mere na glaze. Akara akwụkwọ ma ọ bụ tape na-adapụkarị mgbe ha mịrị mmiri, glaze jupụtakwara na mmiri. Ọ bụ ihe dị mfe ịkpụchapụ akara na-adịghịzi metụta arịa.

    Mkpado: ụzọ ọrụ, ihe ize ndụ, nchekwa
  • Epsom salts

    Obere epsom salts, ngaji ukwu 1 - 2 maka 20 lbs., ga-ejide mkpụrụ glaze n'ime mmiri ma gbochie ka ọ ghara ịghọ ihe siri ike n'okpuru bọket.

    Mkpado: glaze ịnọdụ ala, ịgwakọta
  • Taịlị glaze

    Enwere ike ime taịlị glaze nwere oghere 1/4 inch, wee kegide ya n'aka bọket glaze. Enwere ike ịkpụpụta (extrude) taịlị glaze ahụ n'ọkpụrụkpụ ziri ezi iji ṅomie ite gị, tinye ya akara nọmba batch a pịara n'ụrọ ahụ, ma tee ya slip ị kacha hụ n'anya n'ahịrị. Mgbe ahụ ị ga-ahụ ozugbo otu ọ ga-adị. Mee otu ihe ahụ maka ụrọ niile ị na-ejikarị ka i nwee ọtụtụ ihe ga-ekwe omume n'aka gị.

    Mkpado: taịlị glaze, taịlị, akara
  • Kiln sitter

    Mgbe i tinyechara cone na kiln sitter, jiri masking tape kpuchie ya. Tape ahụ ga-echebe cone ahụ ka a ghara ịkụpụ ya mgbe ị na-etinye ite, ọ na-ere ọkụ pụọ nke ọma mgbe a na-agba ọkụ.

    Mkpado: kiln sitter, cone, cones, itinye ite na kiln