Talooyin glaze
Talooyin wax ku ool ah oo ku saabsan isku-darka, glaze-saarka iyo gubidda, iyo talooyinkaaga.
Talooyin guud
Yeelo nidaam
Habka shaqadaada u yeel nidaam. Waxa aad samayso si joogto ah u qor, diiwaannadana meel wada dhig. Samaynta nidaam wanaagsan oo glaze-ka marinta iyo isku-darka ah waxay yaraynaysaa waqtiga, dadaalka iyo khaladaadka.
Calaamado: nidaam, habab, diiwaannoCuleyska gaarka ah (specific gravity)
Isku-darka glaze-yadaada cufnaan joogto ah, ama culeys gaar ah (specific gravity), aad ayay kuu caawinaysaa gaaritaanka hadafyadaada. Qor cabbirka (cufnaanta ama culeyska gaarka ah) si aad ula socoto saameynta isbeddellada.
Calaamado: culeyska gaarka ah, specific gravity, cufnaan, isku-darGubidda bisque
Samee jadwal gubid bisque oo joogto ah, cone-ka iyo xawaaraha labadaba. Tani waxay u dejinaysaa weelashaada saldhig si ay u yeeshaan heer nuugid glaze oo caadi ah. Yaraynta kala-duwanaanshaha qaybtan habka shaqada waxay kaa caawinaysaa sahaminta iyo xakameynta glaze-yada.
Calaamado: gubidda bisque, bisque firing, bisc firing, bisque-firing, diyaarin, hababWeligaa ha xaaqin
Weligaa ha xaaqin istuudiyaha ama qolka glaze-ka. Habka ugu fiican ee sagxadda loo nadiifiyo waa masaxaad qoyan (mop). Isbuunyo qandaraasle (contractor sponge) ayaa si fiican ugu shaqaynaysa meel leh lakab adag. Boodhku waa natiijo aan laga maarmin oo shaqada dhoobada iyo walxaha glaze-ka, xaaqiddana way kiciysaa.
Calaamado: boodh, khataro, nadaafadda gurigaCalaamado joogto ah
Isticmaal calaamado joogto ah walxaha glaze-ka iyo weelasha glaze-ka. Tani labanlaab ayay muhiim ugu tahay walxaha khatarta ah, oo ku badan midabeeyayaasha glaze-ka sidaas darteedna glaze-yada. Calaamadaha waraaqda ama cajaladda waxay u badan yihiin inay ka dhacaan marka ay qoymaan, glaze-yaduna biyo ayay ka buuxaan. Waa wax fudud in la tirtiro calaamad aan hadda weelka khuseyn.
Calaamado: habab, khataro, kaydinEpsom salts
Xaddi yar oo epsom salts ah, 1 - 2 qaaddo weyn 20 lbs. (rodol), ayaa walxaha glaze-ka ku sii haynaya sabbayn waxayna ka hortagaysaa cufan adag oo ku samaysma salka baaldiga.
Calaamado: dejinta glaze-ka, isku-darTest tile-yada glaze-ka
Test tile-yada glaze-ka waxaa lagu samayn karaa god 1/4 inji ah, kadibna lagu xiri karaa gacanta baaldiga glaze-ka. Test tile-ka waxaa lagu soo saari karaa (extrude) dhumuc sax ah si uu ugu ekaado weelashaada, lagu calaamadeyn karaa lambarka batch-ka oo dhoobada lagu riixay, laguna xariiqi karaa slip-yada aad jeceshahay. Markaas hal mar eegid ayaad ku ogaan kartaa waxa saameyntu noqon doonto. Ku celi dhammaan dhoobooyinkaaga caadiga ah si aad faraha ugu hayso noocyo badan oo suurtagal ah.
Calaamado: test tile-yada glaze-ka, tiles, calaamadoKiln sitter
Kaddib markaad cone-ka gelisid kiln sitter-ka, isticmaal masking tape si aad u daboosho. Cajaladdu waxay ka ilaalinaysaa cone-ka inuu dhaco inta dheryaha la rarayo, waxayna si nadiif ah ugu gubataa gubidda.
Calaamado: kiln sitter, cone, cone-yo, rarid