Ku fahimci glaze ɗinku, ba kawai ku haɗa shi ba. Shigar da girke-girke ku ga UMF (unity molecular formula) ɗinsa, rabon silica da alumina da daidaiton flux nan take. Ajiye girke-girkenku, kayan aiki, masu launi, rubuce-rubuce da bayanan gasa wuri ɗaya a cikin littafi na sirri.

Buɗe asusu kyauta

Ba sai kun yi rajista don gwadawa ba · Kyauta kuma buɗaɗɗen tushe · Girke-girkenku na sirri ne

Jerin cone da aka gasa: farin cone a kowace ƙungiya sun lanƙwasa a cikin zafin kiln.
Ƙungiyoyin cone bayan gasa: kowane cone yana lanƙwasa da zarar kiln ya yi isasshen aikin zafi.

Ga yadda yake aiki: tushen celadon na gargajiya

"4321" na Bernard Leach, wanda ake yawan gasawa zuwa cone 10, a sassa ta nauyi.
KayaSassa
Potash Feldspar40
Silica30
Whiting20
Kaolin10

UMF ɗinsa

Flux - R₂O da RO

  • K₂O : 0.264
  • CaO : 0.736

Masu daidaitawa - R₂O₃

  • Al₂O₃ : 0.407

Masu yin gilashi - RO₂

  • SiO₂ : 3.710

Rabon silica da alumina : 9.11

Flux ɗin suna haɗuwa su zama 1, don haka ana iya kwatanta kowane glaze biyu cikin adalci. An lissafa nan a cikin burauzarku da lambar da lissafin ke amfani da ita.

Abin da Glazecalc ke yi

  • UMF nan take

    Ga flux, alumina da silica a cikin UMF, yadda masana sinadaran glaze ke kwatanta girke-girke, da zarar kun shigar da girke-girke.

  • Gyara da maye gurbi

    An daina yin wani kaya? Kwatanta dabarunsu don samun wanda zai maye gurbinsa ya narke iri ɗaya.

  • Littafin aikinku

    Ajiye girke-girke, kayanku, masu launi, rubuce-rubuce da bayanan gasa wuri ɗaya.

  • Koyi yayin da kuke aiki

    Jagorori cikin sauƙaƙan harshe, daga mene ne glaze zuwa gasa shi cikin aminci, suna kusa da lambobin.

Mene ne UMF (unity molecular formula)?

Girke-girken glaze yana faɗin yawan kowane kaya da za a auna. UMF, wanda ake kuma kira dabarar Seger, yana faɗin abin da kayan suke zama a cikin kiln: yawan molecule na kowane oxide, an daidaita su ta yadda flux ɗin za su haɗu su zama ɗaya.

Flux yana sa glaze ya narke, alumina yana ƙara ƙarfin narkakken, silica kuma yana yin gilashin. Kwatanta waɗannan ƙungiyoyi uku yana bayyana dalilin da ya sa wani glaze yake da sheƙi wani kuma marar sheƙi, ko dalilin da ya sa wani yake gudu wani kuma yake tsayawa, kuma yana nuna yadda za a maye gurbin kayan da ba a sayarwa yanzu.