Waxa uu yahay

Nooca
Flux-yo
Xaaladda
Taariikhi
Qaacidada
SiO₂ 79.62%, K₂O 10.53%, CaO 2.8%, P₂O₅ 1.61%, MnO 0.71%, MgO 0.89%, Fe₂O₃ 0.26%, Al₂O₃ 0.27%, Na₂O 0.35%, LOI 2.92%
Sidoo kale loo yaqaan
藁灰, わら灰, warabai, Rice straw ash
Walxo la mid ah
Synthetic Rice-Straw Ash (合成藁灰)
Isha
Guzmán A., Delvasto S., Sánchez E., 'Valorization of rice straw waste: an alternative ceramic raw material', Cerâmica 61 (357), 2015, Table II, process D (XRF) (2015)

Taariikhi: dhoobo-sameeyayaashu waxay samaysan jireen kooda iyagoo gubaya caws bariis, lamana iibiyo walax caadi ah ahaan. Kani waa hal muunad, oo ah caws bariis Colombia ah oo lagu gubay foorno bannaanka ah kadibna lagu kululeeyey 800 °C muddo 2 saacadood ah, aan la dhaqin. Dambaska cawsku wuxuu ku kala duwan yahay cawska, ciidda iyo gubidda: isla daraasaddaas, gubid kulul ayaa siisay silica badan iyo potash yar, dambaska caws bariiska ee Digitalfire wuxuu leeyahay 77.26% SiO₂ laakiin keliya 3.29% K₂O. Chlorine-kiisa 0.59% iyo sulfur-kiisa 1.74% halkan waxaa lagu tiriyaa wax gubidda ku lumay.

Falanqaynta oksaydhka iyo UMF (unity molecular formula)

Glazecalc wuxuu hayaa falanqaynta walaxda Rice-Straw Ash (藁灰) oo ah boqolkiiba miisaanka walaxda ceeriin. Qaybta UMF waa moles-ka oksaydh kasta ee ku jira xaddiga walaxda Rice-Straw Ash (藁灰) ee haysta 1.0 mole oo flux ah, taasina waa sida Glazecalc ugu daro UMF-ta habka.

Oksaydhyada ku jira walaxda Rice-Straw Ash (藁灰)
Oksaydh Miisaan % Qaybta UMF
SiO₂79.626.644
K₂O10.530.560
CaO2.80.250
P₂O₅1.610.057
MnO0.710.050
MgO0.890.111
Fe₂O₃0.260.008
Al₂O₃0.270.013
Na₂O0.350.028
Miisaanka u dhigma (equivalent weight)
501.36
Miisaanka kaddib gubidda
486.72
LOI (lumista gubidda)
2.92%

Miisaanka u dhigma waa garaamada walaxda Rice-Straw Ash (藁灰) ee haysta 1.0 mole oo flux ah. Miisaanka kaddib gubidda waa inta ka hadha kaddib gubidda.

Khataraha iyo badbaadada

Khataraha: Wuxuu ka kooban yahay silica kiristaalka ah, dambaska aan la dhaqinna wuu gubaa maqaarka (caustic) marka uu qoyan yahay; xiro gacmo-gashi oo ka fogow neefsashada boodhka.

Glazecalc wuxuu muujiyaa qoraalka khatarta sida diiwaanka maktabaddu u bixiyo. Ma aha qiimayn khatar oo dhammaystiran, sidaas darteed akhri warqadda xogta badbaadada (SDS) ee alaab-qeybiyahaaga. Ka hor intaadan taaban walax glaze kasta, akhri Isku-darka ammaanka ah iyo hawo-wareejinta iyo Ha sumayn qoyskaaga.

Ku isticmaal hab

Ku dar walaxda Rice-Straw Ash (藁灰) hab ku jira xisaabiyaha Glazecalc si aad u aragto waxa ay ku samayso UMF-ta glaze-ka.

Fur xisaabiyaha habkaDhammaan walxaha caadiga ah

Samee akoon bilaash ah