Rice-Straw Ash (藁灰)
Okokwakha okujwayelekile kumtapo we-Glazecalc: ukuhlaziywa kwako kwe-oxide, isabelo se-unity nezingozi.
Kuyini
- Uhlobo
- Ama-flux
- Isimo
- Okomlando
- I-formula
- SiO₂ 79.62%, K₂O 10.53%, CaO 2.8%, P₂O₅ 1.61%, MnO 0.71%, MgO 0.89%, Fe₂O₃ 0.26%, Al₂O₃ 0.27%, Na₂O 0.35%, LOI 2.92%
- Kubizwa nangokuthi
- 藁灰, わら灰, warabai, Rice straw ash
- Okokwakha okufanayo
- Synthetic Rice-Straw Ash (合成藁灰)
- Umthombo
- Guzmán A., Delvasto S., Sánchez E., 'Valorization of rice straw waste: an alternative ceramic raw material', Cerâmica 61 (357), 2015, Table II, process D (XRF) (2015)
Okomlando: ababumbi babezenzela owabo ngokushisa izinhlanga zelayisi, futhi awuthengiswa njengokokwakha okujwayelekile. Lesi yisampula esisodwa, sezinhlanga zelayisi zaseColombia ezashiswa esithandweni sangaphandle bese zishiswa ku-800 °C amahora angu-2, zingagezwanga. Umlotha wezinhlanga uyahluka ngokwezinhlanga, inhlabathi nokushiswa: ocwaningweni olufanayo, ukushisa okushisa kakhulu kwanikeza i-silica eningi ne-potash encane, futhi umlotha wezinhlanga zelayisi we-Digitalfire une-77.26% SiO₂ kodwa u-3.29% K₂O kuphela. I-chlorine yawo engu-0.59% ne-sulfur engu-1.74% kubalwa lapha njengokulahleka ekushiseni.
Ukuhlaziywa kwe-oxide ne-unity formula
I-Glazecalc inokuhlaziywa kwe-Rice-Straw Ash (藁灰) njengephesenti lesisindo sokokwakha okuluhlaza. Isabelo se-unity singama-mole e-oxide ngayinye enanini le-Rice-Straw Ash (藁灰) eliqukethe i-mole engu-1.0 ye-flux, okuyindlela i-Glazecalc eyengeza ngayo ku-unity formula yeresiphi.
| I-oxide | Isisindo % | Isabelo se-unity |
|---|---|---|
| SiO₂ | 79.62 | 6.644 |
| K₂O | 10.53 | 0.560 |
| CaO | 2.8 | 0.250 |
| P₂O₅ | 1.61 | 0.057 |
| MnO | 0.71 | 0.050 |
| MgO | 0.89 | 0.111 |
| Fe₂O₃ | 0.26 | 0.008 |
| Al₂O₃ | 0.27 | 0.013 |
| Na₂O | 0.35 | 0.028 |
- Isisindo esilinganayo
- 501.36
- Isisindo esishisiwe
- 486.72
- I-loss on ignition
- 2.92%
Isisindo esilinganayo singamagremu e-Rice-Straw Ash (藁灰) aqukethe i-mole engu-1.0 ye-flux. Isisindo esishisiwe yilokho okusalayo kulokho ngemva kokushisa.
Izingozi nokuphepha
Izingozi: Iqukethe i-silica eyikristalu, futhi umlotha ongagezwanga uyashisa isikhumba (caustic) uma umanzi; gqoka amagilavu futhi ugweme ukuhogela uthuli.
Kusebenzise eresiphini
Engeza i-Rice-Straw Ash (藁灰) eresiphini ku-calculator ye-Glazecalc ukuze ubone ukuthi yenzani ku-unity formula ye-glaze.