Rice-Straw Ash (藁灰)
Ihe a na-ejikarị n'ọbá akwụkwọ Glazecalc: nyocha oxide ya, ntinye unity ya na ihe ize ndụ ya.
Ihe ọ bụ
- Ụdị
- Flux
- Ọnọdụ
- Nke oge gara aga
- Formula
- SiO₂ 79.62%, K₂O 10.53%, CaO 2.8%, P₂O₅ 1.61%, MnO 0.71%, MgO 0.89%, Fe₂O₃ 0.26%, Al₂O₃ 0.27%, Na₂O 0.35%, LOI 2.92%
- A na-akpọkwa ya
- 藁灰, わら灰, warabai, Rice straw ash
- Ihe ndị yiri ya
- Synthetic Rice-Straw Ash (合成藁灰)
- Ebe o si
- Guzmán A., Delvasto S., Sánchez E., 'Valorization of rice straw waste: an alternative ceramic raw material', Cerâmica 61 (357), 2015, Table II, process D (XRF) (2015)
Akụkọ ihe mere eme: ndị ọkpụ ite na-eme nke ha site n'ịgba ahịhịa osikapa ọkụ, a naghịkwa ere ya dịka ihe nkịtị. Nke a bụ otu nlele, nke ahịhịa osikapa Colombia a gbara ọkụ n'ọkụ dị n'èzí emesịa kpoo ya ọkụ ruo 800 °C ruo awa 2, a saghị ya. Ntụ ahịhịa na-adịgasị iche dabere n'ahịhịa, ala na ịgba ọkụ: n'otu nnyocha ahụ, ịgba ọkụ dị ọkụ karịa nyere silica karịa na potash pere mpe, ntụ ahịhịa osikapa nke Digitalfire nwekwara SiO₂ 77.26% mana naanị K₂O 3.29%. A na-agụ chlorine ya nke 0.59% na sulfur nke 1.74% ebe a dịka ihe furu efu n'ọkụ.
Nyocha oxide na unity formula
Glazecalc nwere nyocha Rice-Straw Ash (藁灰) dịka pasent ịdị arọ nke ihe ahụ a na-agbabeghị ọkụ. Ntinye unity bụ moles nke oxide ọ bụla n'ọnụ ọgụgụ Rice-Straw Ash (藁灰) nke nwere 1.0 mole nke flux; otu a ka Glazecalc si agbakwunye ya n'unity formula nke usoro.
| Oxide | Ịdị arọ % | Ntinye unity |
|---|---|---|
| SiO₂ | 79.62 | 6.644 |
| K₂O | 10.53 | 0.560 |
| CaO | 2.8 | 0.250 |
| P₂O₅ | 1.61 | 0.057 |
| MnO | 0.71 | 0.050 |
| MgO | 0.89 | 0.111 |
| Fe₂O₃ | 0.26 | 0.008 |
| Al₂O₃ | 0.27 | 0.013 |
| Na₂O | 0.35 | 0.028 |
- Ịdị arọ nhata (equivalent weight)
- 501.36
- Ịdị arọ mgbe a gbara ọkụ
- 486.72
- Loss on ignition (LOI)
- 2.92%
Ịdị arọ nhata bụ grams nke Rice-Straw Ash (藁灰) nke nwere 1.0 mole nke flux. Ịdị arọ mgbe a gbara ọkụ bụ ihe fọdụrụ na ya mgbe a gbachara ọkụ.
Ihe ize ndụ na nchekwa
Ihe ize ndụ: O nwere crystalline silica, ntụ a saghị asa na-ere akpụkpọ ahụ (caustic) mgbe ọ dị mmiri; yiri uwe aka ma zere iku uzuzu ahụ ume.
Jiri ya n'usoro
Tinye Rice-Straw Ash (藁灰) n'usoro na Glazecalc calculator ka ị hụ ihe ọ na-eme unity formula nke glaze.