Wood Ash (average of six)
Kayan aiki na asali a laburaren Glazecalc: binciken oxide ɗinsa, gudummawar UMF da haɗarinsa.
Mene ne shi
- Nau’i
- Flux (masu narkarwa)
- Matsayi
- Na tarihi
- Tsarin sinadarai
- CaO 37%, MgO 11%, K₂O 16%, Na₂O 1%, P₂O₅ 9%, SiO₂ 7%, Fe₂O₃ 1%, MnO 2%, LOI 16%
- Ana kuma kiransa
- Wood ash, 木灰
- Kayan aiki masu kama
- Synthetic Wood Ash (合成土灰)
- Tushe
- Digitalfire Reference Library: Wood Ash (an average of 6 wood ash types) (2026-11-04)
Na tarihi: maginan tukwane suna ƙona itacensu sannan su wanke tokar a ruwa, suna zubar da gawayin da ke yawo, ko kuma su tace ta a bushe, wanda ke riƙe potash da soda masu narkewa a ruwa. Wannan matsakaicin Digitalfire ne na tokar itace shida, ba toka ɗaya ba: toka ta gaske tana bambanta daga itace zuwa itace da kuma daga batch zuwa batch, don haka ku gwada taku, misali a line blend tare da feldspar.
Binciken oxide da UMF
Glazecalc yana da binciken Wood Ash (average of six) a matsayin kashi bisa nauyi na ɗanyen kayan. Gudummawar UMF ita ce mole na kowane oxide a cikin adadin Wood Ash (average of six) da ke ɗauke da mole 1.0 na flux, kuma haka Glazecalc ke ƙara shi cikin UMF (unity molecular formula) na tsarin glaze.
| Oxide | Kashi bisa nauyi % | Gudummawar UMF |
|---|---|---|
| CaO | 37 | 0.575 |
| MgO | 11 | 0.238 |
| K₂O | 16 | 0.148 |
| Na₂O | 1 | 0.014 |
| P₂O₅ | 9 | 0.055 |
| SiO₂ | 7 | 0.102 |
| Fe₂O₃ | 1 | 0.005 |
| MnO | 2 | 0.025 |
- Nauyin daidai (equivalent weight)
- 87.19
- Nauyi bayan gasa
- 73.24
- LOI (raguwar nauyi a wuta)
- 16%
Nauyin daidai shi ne giram na Wood Ash (average of six) da ke ɗauke da mole 1.0 na flux. Nauyi bayan gasa shi ne abin da ya rage daga wannan bayan gasa.
Haɗari da tsaro
Haɗari: Tokar itace tana ƙona fata (caustic), haka ma ruwan da ake wanke ta da shi: ku sa safar hannu da kariyar ido, kuma ku guji shaƙar ƙurar.
Yi amfani da shi a tsarin glaze
Ƙara Wood Ash (average of six) cikin tsarin glaze a kalkuletan Glazecalc don ganin abin da yake yi wa UMF na glaze.