Ihe ọ bụ

Ụdị
Flux
Ọnọdụ
Nke oge gara aga
Formula
CaO 37%, MgO 11%, K₂O 16%, Na₂O 1%, P₂O₅ 9%, SiO₂ 7%, Fe₂O₃ 1%, MnO 2%, LOI 16%
A na-akpọkwa ya
Wood ash, 木灰
Ihe ndị yiri ya
Synthetic Wood Ash (合成土灰)
Ebe o si
Digitalfire Reference Library: Wood Ash (an average of 6 wood ash types) (2026-11-04)

Akụkọ ihe mere eme: ndị ọkpụ ite na-agba osisi nke ha ọkụ ma sachaa ntụ ahụ na mmiri, na-awụpụ unyi na-ese n'elu, ma ọ bụ nyọọ ya mgbe ọ kpọrọ nkụ, nke na-echekwa potash na soda na-agbaze na mmiri. Nke a bụ nkezi Digitalfire nke ntụ osisi isii, ọ bụghị otu ntụ: ezigbo ntụ na-adịgasị iche site n'osisi ruo osisi na site na batch ruo batch, ya mere nwalee nke gị, dịka ọmụmaatụ na line blend ya na feldspar.

Nyocha oxide na unity formula

Glazecalc nwere nyocha Wood Ash (average of six) dịka pasent ịdị arọ nke ihe ahụ a na-agbabeghị ọkụ. Ntinye unity bụ moles nke oxide ọ bụla n'ọnụ ọgụgụ Wood Ash (average of six) nke nwere 1.0 mole nke flux; otu a ka Glazecalc si agbakwunye ya n'unity formula nke usoro.

Oxide dị na Wood Ash (average of six)
Oxide Ịdị arọ % Ntinye unity
CaO370.575
MgO110.238
K₂O160.148
Na₂O10.014
P₂O₅90.055
SiO₂70.102
Fe₂O₃10.005
MnO20.025
Ịdị arọ nhata (equivalent weight)
87.19
Ịdị arọ mgbe a gbara ọkụ
73.24
Loss on ignition (LOI)
16%

Ịdị arọ nhata bụ grams nke Wood Ash (average of six) nke nwere 1.0 mole nke flux. Ịdị arọ mgbe a gbara ọkụ bụ ihe fọdụrụ na ya mgbe a gbachara ọkụ.

Ihe ize ndụ na nchekwa

Ihe ize ndụ: Ntụ osisi na-ere akpụkpọ ahụ (caustic), otu ahụkwa ka mmiri a na-eji asa ya dị: yiri uwe aka na ihe nchebe anya, ma zere iku uzuzu ahụ ume.

Glazecalc na-egosi okwu ihe ize ndụ dịka ndekọ ọbá akwụkwọ si dee ya. Ọ bụghị nyocha ihe ize ndụ zuru ezu, ya mere gụọ mpempe data nchekwa site n'aka onye na-ere gị ya. Tupu i metụ ihe glaze ọ bụla, gụọ Ịgwakọta n'enweghị ihe ize ndụ na ikuku dị ọcha na Enyela ezinụlọ gị nsí.

Jiri ya n'usoro

Tinye Wood Ash (average of six) n'usoro na Glazecalc calculator ka ị hụ ihe ọ na-eme unity formula nke glaze.

Mepee calculator usoroIhe niile a na-ejikarị

Mepụta akaụntụ n'efu