Wood Ash (average of six)
Okokwakha okujwayelekile kumtapo we-Glazecalc: ukuhlaziywa kwako kwe-oxide, isabelo se-unity nezingozi.
Kuyini
- Uhlobo
- Ama-flux
- Isimo
- Okomlando
- I-formula
- CaO 37%, MgO 11%, K₂O 16%, Na₂O 1%, P₂O₅ 9%, SiO₂ 7%, Fe₂O₃ 1%, MnO 2%, LOI 16%
- Kubizwa nangokuthi
- Wood ash, 木灰
- Okokwakha okufanayo
- Synthetic Wood Ash (合成土灰)
- Umthombo
- Digitalfire Reference Library: Wood Ash (an average of 6 wood ash types) (2026-11-04)
Okomlando: ababumbi babeshisa izinkuni zabo bese begeza umlotha emanzini, bethela amalahle antantayo, noma bawuhlunga womile, okugcina i-potash ne-soda ezincibilika emanzini. Lesi yisilinganiso se-Digitalfire semilotha yezinkuni eyisithupha, hhayi umlotha owodwa: umlotha wangempela uyahluka kusuka ezinkunini ziye kwezinye nakusuka ku-batch kuye kwenye, ngakho hlola owakho, ngokwesibonelo ku-line blend ne-feldspar.
Ukuhlaziywa kwe-oxide ne-unity formula
I-Glazecalc inokuhlaziywa kwe-Wood Ash (average of six) njengephesenti lesisindo sokokwakha okuluhlaza. Isabelo se-unity singama-mole e-oxide ngayinye enanini le-Wood Ash (average of six) eliqukethe i-mole engu-1.0 ye-flux, okuyindlela i-Glazecalc eyengeza ngayo ku-unity formula yeresiphi.
| I-oxide | Isisindo % | Isabelo se-unity |
|---|---|---|
| CaO | 37 | 0.575 |
| MgO | 11 | 0.238 |
| K₂O | 16 | 0.148 |
| Na₂O | 1 | 0.014 |
| P₂O₅ | 9 | 0.055 |
| SiO₂ | 7 | 0.102 |
| Fe₂O₃ | 1 | 0.005 |
| MnO | 2 | 0.025 |
- Isisindo esilinganayo
- 87.19
- Isisindo esishisiwe
- 73.24
- I-loss on ignition
- 16%
Isisindo esilinganayo singamagremu e-Wood Ash (average of six) aqukethe i-mole engu-1.0 ye-flux. Isisindo esishisiwe yilokho okusalayo kulokho ngemva kokushisa.
Izingozi nokuphepha
Izingozi: Umlotha wezinkuni uyashisa isikhumba (caustic), kanjalo namanzi ogezwa ngawo: gqoka amagilavu nesivikelo samehlo, futhi ugweme ukuhogela uthuli.
Kusebenzise eresiphini
Engeza i-Wood Ash (average of six) eresiphini ku-calculator ye-Glazecalc ukuze ubone ukuthi yenzani ku-unity formula ye-glaze.