Mene ne shi

Nau’i
Flux (masu narkarwa)
Tsarin sinadarai
SiO₂ 17.34%, Al₂O₃ 3.45%, Fe₂O₃ 0.33%, CaO 36.09%, MgO 5.88%, Na₂O 0.02%, K₂O 0.15%, LOI 36.74%
Ana kuma kiransa
合成土灰, gōsei dobai, Synthetic dobai
Ana sayar da shi a
JP
Tushe
佐賀県陶磁器原料株式会社 (Arita): 釉薬原料の化学分析表, the supplier's typical analysis of what it sells (undated; read 2026-11-04). Second analysis: 吉田博和ほか「笠間焼の新素地・新釉薬の開発」, 茨城県工業技術センター研究報告 43 (2014), 表6

Nazari na yau da kullum daga mai sayarwa ɗaya a Arita: kwatanta shi da na mai sayar muku. Madadin da aka ƙera (synthetic) na 土灰, gauraye tokar itace ta glaze na toka na Japan; ba toka ta gaske ba ce, wadda take bambanta sosai. Adadin mai sayarwar ya kai 96.45%, don haka 3.55% da suka bari ana ƙirga shi a nan a matsayin abin da ya ɓace a gasa, tare da LOI ɗinsa na 33.19%. Nazarin 2014 na cibiyar fasahar masana'antu ta Ibaraki na wani 合成土灰 ya kusan zama ɗaya: SiO₂ 18.2%, CaO 33.6%, MgO 8.1%, LOI 33.8%.

Binciken oxide da UMF

Glazecalc yana da binciken Synthetic Wood Ash (合成土灰) a matsayin kashi bisa nauyi na ɗanyen kayan. Gudummawar UMF ita ce mole na kowane oxide a cikin adadin Synthetic Wood Ash (合成土灰) da ke ɗauke da mole 1.0 na flux, kuma haka Glazecalc ke ƙara shi cikin UMF (unity molecular formula) na tsarin glaze.

Oxide a cikin Synthetic Wood Ash (合成土灰)
Oxide Kashi bisa nauyi % Gudummawar UMF
SiO₂17.340.365
Al₂O₃3.450.043
Fe₂O₃0.330.003
CaO36.090.813
MgO5.880.184
Na₂O0.020.000
K₂O0.150.002
Nauyin daidai (equivalent weight)
126.36
Nauyi bayan gasa
79.94
LOI (raguwar nauyi a wuta)
36.74%

Nauyin daidai shi ne giram na Synthetic Wood Ash (合成土灰) da ke ɗauke da mole 1.0 na flux. Nauyi bayan gasa shi ne abin da ya rage daga wannan bayan gasa.

Haɗari da tsaro

Haɗari: Ku guji shaƙar ƙurar.

Glazecalc yana nuna kalmomin haɗari kamar yadda bayanin laburaren ya ba da su. Wannan ba cikakken kimanta haɗari ba ne, don haka ku karanta takardar bayanan aminci daga mai sayar muku. Kafin ku taɓa kowane kayan glaze, ku karanta Haɗawa cikin aminci da iska mai kyau da Kada ka sa wa iyalinka guba.

Yi amfani da shi a tsarin glaze

Ƙara Synthetic Wood Ash (合成土灰) cikin tsarin glaze a kalkuletan Glazecalc don ganin abin da yake yi wa UMF na glaze.

Buɗe kalkuletan tsarin glazeDuk kayan aiki na asali

Buɗe asusu kyauta