Imataq kay

Laya
Fundentekuna
Fórmula
SiO₂ 17.34%, Al₂O₃ 3.45%, Fe₂O₃ 0.33%, CaO 36.09%, MgO 5.88%, Na₂O 0.02%, K₂O 0.15%, LOI 36.74%
Huk sutinkuna
合成土灰, gōsei dobai, Synthetic dobai
Maypi rantikun
JP
Fuente
佐賀県陶磁器原料株式会社 (Arita): 釉薬原料の化学分析表, the supplier's typical analysis of what it sells (undated; read 2026-11-04). Second analysis: 吉田博和ほか「笠間焼の新素地・新釉薬の開発」, 茨城県工業技術センター研究報告 43 (2014), 表6

Arita llaqtapi huk qhatuqpa sapa kuti análisisnin: qampa qhatuqniykipa análisisninwan tupachiy. 土灰 nisqapa ruranasqa (sintético) rantinmi, Japónpa uchpa esmaltenkunap chaqrusqa k'aspi uchpan; manam chiqaq uchpachu, chiqaq uchpaqa ancha hukniraqmi. Qhatuqpa yupayninkunaqa 96.45%-mi, chayrayku saqisqanku 3.55%-qa kaypi ruphachiypi chinkasqa hina yupakun, 33.19% LOI-nwan. 2014 watapi Ibarakip industria tecnología centronpa huk 合成土灰 análisisninqa yaqa kaqllam karqan: SiO₂ 18.2%, CaO 33.6%, MgO 8.1%, LOI 33.8%.

Óxido análisis, fórmula unitaria ima

Glazecalcqa material Synthetic Wood Ash (合成土灰) sutiyuqpa análisisninta mana ruphachisqa materialpa llasayninpi porcentaje hina hap'in. Fórmula unitariaman yapayninqa sapa óxidopa molninkunam, chay materialpa 1.0 mol fundenteta hap'iq kaqninpi; chaywanmi Glazecalc esmalte ruranapa fórmula unitarianman yapan.

Material Synthetic Wood Ash (合成土灰) sutiyuqpi óxidokuna
Óxido Llasay % Fórmula unitariaman yapaynin
SiO₂17.340.365
Al₂O₃3.450.043
Fe₂O₃0.330.003
CaO36.090.813
MgO5.880.184
Na₂O0.020.000
K₂O0.150.002
Peso equivalente
126.36
Ruphachisqa peso
79.94
Ruphachiypi chinkaq (LOI)
36.74%

Peso equivalenteqa material Synthetic Wood Ash (合成土灰) sutiyuqpa gramonkunam, 1.0 mol fundenteta hap'iq. Ruphachisqa pesoqa chaymanta ruphachisqa qhipa puchuqmi.

Peligrokuna, seguridad ima

Peligrokuna: Ñut'u allpa samaykuymanta karunchakuy.

Glazecalcqa peligro simikunata qillqa wasipa registron qusqan hinam rikuchin. Manam hunt'asqa peligro tupuychu, chaymi qhatuqniykipa seguridad datos p'anqanta ñawinchay. Mayqin esmalte materialtapas manaraq hap'ispa, Mana manchakuspa chaqruy, wayra puriynin, Ama ayllu-masiykita miyuwan wañuchiychu ima qillqakunata ñawinchay.

Esmalte ruranapi apaykachay

Material Synthetic Wood Ash (合成土灰) sutiyuqta Glazecalc calculadorapi huk esmalte ruranaman yapay, esmaltepa fórmula unitarianta imayna cambiachisqanta rikunaykipaq.

Esmalte rurana calculadorata kichayTukuy estándar materialkuna

Mana qullqiyuq cuentata kichay