Synthetic Wood Ash (合成土灰)
Walax caadi ah oo ku jirta maktabadda Glazecalc: falanqaynta oksaydhka, qaybta UMF iyo khataraha.
Waxa uu yahay
- Nooca
- Flux-yo
- Qaacidada
- SiO₂ 17.34%, Al₂O₃ 3.45%, Fe₂O₃ 0.33%, CaO 36.09%, MgO 5.88%, Na₂O 0.02%, K₂O 0.15%, LOI 36.74%
- Sidoo kale loo yaqaan
- 合成土灰, gōsei dobai, Synthetic dobai
- Waxaa lagu iibiyaa
- JP
- Isha
- 佐賀県陶磁器原料株式会社 (Arita): 釉薬原料の化学分析表, the supplier's typical analysis of what it sells (undated; read 2026-11-04). Second analysis: 吉田博和ほか「笠間焼の新素地・新釉薬の開発」, 茨城県工業技術センター研究報告 43 (2014), 表6
Falanqayn caadi ah oo ka timid hal iibiye oo Arita ku sugan: barbardhig tan iibiyahaaga. Beddel la sameeyey (synthetic) oo loogu talagalay 土灰, dambaska qoryaha isku dhafan ee glaze-yada dambaska Japan; ma aha dambas dhab ah, kaas oo aad u kala duwan. Tirooyinka iibiyuhu waxay isku gaarayaan 96.45%, sidaa darteed 3.55% ay ka tageen halkan waxaa lagu tiriyaa wax gubidda ku lumay, oo leh LOI-giisa 33.19%. Falanqayn 2014 ah oo xarunta tiknoolajiyada warshadaha Ibaraki ku samaysay 合成土灰 kale ayaa ku dhowaad la mid ahayd: SiO₂ 18.2%, CaO 33.6%, MgO 8.1%, LOI 33.8%.
Falanqaynta oksaydhka iyo UMF (unity molecular formula)
Glazecalc wuxuu hayaa falanqaynta walaxda Synthetic Wood Ash (合成土灰) oo ah boqolkiiba miisaanka walaxda ceeriin. Qaybta UMF waa moles-ka oksaydh kasta ee ku jira xaddiga walaxda Synthetic Wood Ash (合成土灰) ee haysta 1.0 mole oo flux ah, taasina waa sida Glazecalc ugu daro UMF-ta habka.
| Oksaydh | Miisaan % | Qaybta UMF |
|---|---|---|
| SiO₂ | 17.34 | 0.365 |
| Al₂O₃ | 3.45 | 0.043 |
| Fe₂O₃ | 0.33 | 0.003 |
| CaO | 36.09 | 0.813 |
| MgO | 5.88 | 0.184 |
| Na₂O | 0.02 | 0.000 |
| K₂O | 0.15 | 0.002 |
- Miisaanka u dhigma (equivalent weight)
- 126.36
- Miisaanka kaddib gubidda
- 79.94
- LOI (lumista gubidda)
- 36.74%
Miisaanka u dhigma waa garaamada walaxda Synthetic Wood Ash (合成土灰) ee haysta 1.0 mole oo flux ah. Miisaanka kaddib gubidda waa inta ka hadha kaddib gubidda.
Khataraha iyo badbaadada
Khataraha: Ka fogow neefsashada boodhka.
Ku isticmaal hab
Ku dar walaxda Synthetic Wood Ash (合成土灰) hab ku jira xisaabiyaha Glazecalc si aad u aragto waxa ay ku samayso UMF-ta glaze-ka.