Masuda Feldspar (益田長石)
Kayan aiki na asali a laburaren Glazecalc: binciken oxide ɗinsa, gudummawar UMF da haɗarinsa.
Mene ne shi
- Nau’i
- Feldspar da duwatsu
- Tsarin sinadarai
- SiO₂ 66.32%, Al₂O₃ 18.59%, Fe₂O₃ 0.07%, CaO 0.06%, MgO 0.04%, Na₂O 3.26%, K₂O 10.35%, LOI 0.9%
- Ana kuma kiransa
- 益田長石, Masuda feldspar
- Ana sayar da shi a
- JP
- Tushe
- 佐賀県陶磁器原料株式会社 (Arita): 釉薬原料の化学分析表, the supplier's typical analysis of what it sells (undated; read 2026-11-04)
Nazari na yau da kullum daga mai sayarwa ɗaya a Arita: kwatanta shi da na mai sayar muku. Feldspar na potash, mai K₂O 10.35%; an ba da TiO₂ ne kawai a matsayin ɗan kaɗan. Mai sayarwar guda yana sayar da wani nau'i daban, 益田長石 F-1, wanda ba a yi nazarinsa a nan ba.
Binciken oxide da UMF
Glazecalc yana da binciken Masuda Feldspar (益田長石) a matsayin kashi bisa nauyi na ɗanyen kayan. Gudummawar UMF ita ce mole na kowane oxide a cikin adadin Masuda Feldspar (益田長石) da ke ɗauke da mole 1.0 na flux, kuma haka Glazecalc ke ƙara shi cikin UMF (unity molecular formula) na tsarin glaze.
| Oxide | Kashi bisa nauyi % | Gudummawar UMF |
|---|---|---|
| SiO₂ | 66.32 | 6.708 |
| Al₂O₃ | 18.59 | 1.108 |
| Fe₂O₃ | 0.07 | 0.003 |
| CaO | 0.06 | 0.007 |
| MgO | 0.04 | 0.006 |
| Na₂O | 3.26 | 0.320 |
| K₂O | 10.35 | 0.668 |
- Nauyin daidai (equivalent weight)
- 607.76
- Nauyi bayan gasa
- 602.29
- LOI (raguwar nauyi a wuta)
- 0.9%
Nauyin daidai shi ne giram na Masuda Feldspar (益田長石) da ke ɗauke da mole 1.0 na flux. Nauyi bayan gasa shi ne abin da ya rage daga wannan bayan gasa.
Haɗari da tsaro
Haɗari: Yana ƙunshe da crystalline silica; ku guji shaƙar ƙurar.
Yi amfani da shi a tsarin glaze
Ƙara Masuda Feldspar (益田長石) cikin tsarin glaze a kalkuletan Glazecalc don ganin abin da yake yi wa UMF na glaze.