Masuda Feldspar (益田長石)
Ihe a na-ejikarị n'ọbá akwụkwọ Glazecalc: nyocha oxide ya, ntinye unity ya na ihe ize ndụ ya.
Ihe ọ bụ
- Ụdị
- Feldspar na nkume
- Formula
- SiO₂ 66.32%, Al₂O₃ 18.59%, Fe₂O₃ 0.07%, CaO 0.06%, MgO 0.04%, Na₂O 3.26%, K₂O 10.35%, LOI 0.9%
- A na-akpọkwa ya
- 益田長石, Masuda feldspar
- A na-ere ya na
- JP
- Ebe o si
- 佐賀県陶磁器原料株式会社 (Arita): 釉薬原料の化学分析表, the supplier's typical analysis of what it sells (undated; read 2026-11-04)
Nyocha a na-ahụkarị site n'aka otu onye na-ere ahịa na Arita: tụnyere ya na nke onye na-ere gị. Feldspar potash, nwere K₂O 10.35%; e nyere TiO₂ naanị dịka obere ntakịrị. Otu onye na-ere ahịa ahụ na-ere ọkwa ọzọ dị iche, 益田長石 F-1, nke a nyochaghị ebe a.
Nyocha oxide na unity formula
Glazecalc nwere nyocha Masuda Feldspar (益田長石) dịka pasent ịdị arọ nke ihe ahụ a na-agbabeghị ọkụ. Ntinye unity bụ moles nke oxide ọ bụla n'ọnụ ọgụgụ Masuda Feldspar (益田長石) nke nwere 1.0 mole nke flux; otu a ka Glazecalc si agbakwunye ya n'unity formula nke usoro.
| Oxide | Ịdị arọ % | Ntinye unity |
|---|---|---|
| SiO₂ | 66.32 | 6.708 |
| Al₂O₃ | 18.59 | 1.108 |
| Fe₂O₃ | 0.07 | 0.003 |
| CaO | 0.06 | 0.007 |
| MgO | 0.04 | 0.006 |
| Na₂O | 3.26 | 0.320 |
| K₂O | 10.35 | 0.668 |
- Ịdị arọ nhata (equivalent weight)
- 607.76
- Ịdị arọ mgbe a gbara ọkụ
- 602.29
- Loss on ignition (LOI)
- 0.9%
Ịdị arọ nhata bụ grams nke Masuda Feldspar (益田長石) nke nwere 1.0 mole nke flux. Ịdị arọ mgbe a gbara ọkụ bụ ihe fọdụrụ na ya mgbe a gbachara ọkụ.
Ihe ize ndụ na nchekwa
Ihe ize ndụ: O nwere crystalline silica; zere iku uzuzu ya.
Jiri ya n'usoro
Tinye Masuda Feldspar (益田長石) n'usoro na Glazecalc calculator ka ị hụ ihe ọ na-eme unity formula nke glaze.