Waxa uu yahay

Nooca
Feldspar iyo dhagxaan
Qaacidada
SiO₂ 66.32%, Al₂O₃ 18.59%, Fe₂O₃ 0.07%, CaO 0.06%, MgO 0.04%, Na₂O 3.26%, K₂O 10.35%, LOI 0.9%
Sidoo kale loo yaqaan
益田長石, Masuda feldspar
Waxaa lagu iibiyaa
JP
Isha
佐賀県陶磁器原料株式会社 (Arita): 釉薬原料の化学分析表, the supplier's typical analysis of what it sells (undated; read 2026-11-04)

Falanqayn caadi ah oo ka timid hal iibiye oo Arita ku sugan: barbardhig tan iibiyahaaga. Feldspar potash ah, oo leh 10.35% K₂O; TiO₂ waxaa la bixiyey keliya raad ahaan. Isla iibiyahaas wuxuu iibiyaa heer kale oo gooni ah, 益田長石 F-1, oo halkan aan lagu falanqayn.

Falanqaynta oksaydhka iyo UMF (unity molecular formula)

Glazecalc wuxuu hayaa falanqaynta walaxda Masuda Feldspar (益田長石) oo ah boqolkiiba miisaanka walaxda ceeriin. Qaybta UMF waa moles-ka oksaydh kasta ee ku jira xaddiga walaxda Masuda Feldspar (益田長石) ee haysta 1.0 mole oo flux ah, taasina waa sida Glazecalc ugu daro UMF-ta habka.

Oksaydhyada ku jira walaxda Masuda Feldspar (益田長石)
Oksaydh Miisaan % Qaybta UMF
SiO₂66.326.708
Al₂O₃18.591.108
Fe₂O₃0.070.003
CaO0.060.007
MgO0.040.006
Na₂O3.260.320
K₂O10.350.668
Miisaanka u dhigma (equivalent weight)
607.76
Miisaanka kaddib gubidda
602.29
LOI (lumista gubidda)
0.9%

Miisaanka u dhigma waa garaamada walaxda Masuda Feldspar (益田長石) ee haysta 1.0 mole oo flux ah. Miisaanka kaddib gubidda waa inta ka hadha kaddib gubidda.

Khataraha iyo badbaadada

Khataraha: Waxaa ku jira silica kiristaal ah; iska ilaali neefsashada boodhka.

Glazecalc wuxuu muujiyaa qoraalka khatarta sida diiwaanka maktabaddu u bixiyo. Ma aha qiimayn khatar oo dhammaystiran, sidaas darteed akhri warqadda xogta badbaadada (SDS) ee alaab-qeybiyahaaga. Ka hor intaadan taaban walax glaze kasta, akhri Isku-darka ammaanka ah iyo hawo-wareejinta iyo Ha sumayn qoyskaaga.

Ku isticmaal hab

Ku dar walaxda Masuda Feldspar (益田長石) hab ku jira xisaabiyaha Glazecalc si aad u aragto waxa ay ku samayso UMF-ta glaze-ka.

Fur xisaabiyaha habkaDhammaan walxaha caadiga ah

Samee akoon bilaash ah