Kuyini

Uhlobo
Ama-feldspar namatshe
I-formula
SiO₂ 66.32%, Al₂O₃ 18.59%, Fe₂O₃ 0.07%, CaO 0.06%, MgO 0.04%, Na₂O 3.26%, K₂O 10.35%, LOI 0.9%
Kubizwa nangokuthi
益田長石, Masuda feldspar
Kuthengiswa e
JP
Umthombo
佐賀県陶磁器原料株式会社 (Arita): 釉薬原料の化学分析表, the supplier's typical analysis of what it sells (undated; read 2026-11-04)

Ukuhlaziywa okujwayelekile okuvela kumphakeli oyedwa e-Arita: kuqhathanise nokomphakeli wakho. I-feldspar ye-potash, ene-10.35% K₂O; i-TiO₂ inikezwa njengokuncane kakhulu kuphela. Umphakeli ofanayo uthengisa izinga elihlukile, i-益田長石 F-1, elingahlaziywanga lapha.

Ukuhlaziywa kwe-oxide ne-unity formula

I-Glazecalc inokuhlaziywa kwe-Masuda Feldspar (益田長石) njengephesenti lesisindo sokokwakha okuluhlaza. Isabelo se-unity singama-mole e-oxide ngayinye enanini le-Masuda Feldspar (益田長石) eliqukethe i-mole engu-1.0 ye-flux, okuyindlela i-Glazecalc eyengeza ngayo ku-unity formula yeresiphi.

Ama-oxide aku-Masuda Feldspar (益田長石)
I-oxide Isisindo % Isabelo se-unity
SiO₂66.326.708
Al₂O₃18.591.108
Fe₂O₃0.070.003
CaO0.060.007
MgO0.040.006
Na₂O3.260.320
K₂O10.350.668
Isisindo esilinganayo
607.76
Isisindo esishisiwe
602.29
I-loss on ignition
0.9%

Isisindo esilinganayo singamagremu e-Masuda Feldspar (益田長石) aqukethe i-mole engu-1.0 ye-flux. Isisindo esishisiwe yilokho okusalayo kulokho ngemva kokushisa.

Izingozi nokuphepha

Izingozi: Kuqukethe i-silica eyikristalu; gwema ukuhogela uthuli.

I-Glazecalc ibonisa amagama engozi njengoba irekhodi lomtapo liwanikeza. Akukona ukuhlolwa okugcwele kwengozi, ngakho funda ishidi lemininingwane yokuphepha elivela kumphakeli wakho. Ngaphambi kokuthi uthinte noma yikuphi okokwakha kwe-glaze, funda Ukuxuba ngokuphepha nomoya ohlanzekile futhi Ungawadliseli ushevu umndeni wakho.

Kusebenzise eresiphini

Engeza i-Masuda Feldspar (益田長石) eresiphini ku-calculator ye-Glazecalc ukuze ubone ukuthi yenzani ku-unity formula ye-glaze.

Vula i-calculator yeresiphiKonke okokwakha okujwayelekile

Vula i-akhawunti yamahhala