Tsarin sinadarai
SiO₂ 66.93%, Al₂O₃ 18.01%, CaO 1.23%, MgO 0.51%, K₂O 5.23%, Na₂O 0.45%, Fe₂O₃ 3.11%, TiO₂ 0.45%, MnO 0.08%, LOI 4.47%
Ana kuma kiransa
Gaojitou Zijin soil, Zijin soil, 紫金土
Kayan aiki masu kama
Redart
Tushe
He Z., Zhang M., Zhang H., 'Data-driven research on chemical features of Jingdezhen and Longquan celadon by energy dispersive X-ray fluorescence', arXiv:1511.07825 (2015), Table 6 (2015)

Na tarihi: yumɓun yanki mai ƙarfe mai yawa (紫金土) daga ƙauyen Gaojitou a Dayao, kusa da kiln na Longquan a China, da ake ƙarawa a cikin yumɓun Longquan saboda ƙarfensa da alumina; ba a sayar da shi a wajen China. Wannan nazari ɗaya ne, wanda takardar ta ɗauko daga binciken China na baya. Yadda aka haƙa shi aka shirya shi ba ya cikin majiyar.

Binciken oxide da UMF

Glazecalc yana da binciken Longquan Zijin Soil, Gaojitou a matsayin kashi bisa nauyi na ɗanyen kayan. Gudummawar UMF ita ce mole na kowane oxide a cikin adadin Longquan Zijin Soil, Gaojitou da ke ɗauke da mole 1.0 na flux, kuma haka Glazecalc ke ƙara shi cikin UMF (unity molecular formula) na tsarin glaze.

Oxide a cikin Longquan Zijin Soil, Gaojitou
Oxide Kashi bisa nauyi % Gudummawar UMF
SiO₂66.9311.309
Al₂O₃18.011.793
CaO1.230.223
MgO0.510.128
K₂O5.230.564
Na₂O0.450.074
Fe₂O₃3.110.198
TiO₂0.450.057
MnO0.080.011
Nauyin daidai (equivalent weight)
1015.24
Nauyi bayan gasa
969.85
LOI (raguwar nauyi a wuta)
4.47%

Nauyin daidai shi ne giram na Longquan Zijin Soil, Gaojitou da ke ɗauke da mole 1.0 na flux. Nauyi bayan gasa shi ne abin da ya rage daga wannan bayan gasa.

Haɗari da tsaro

Haɗari: Yana ƙunshe da crystalline silica; ku guji shaƙar ƙurar.

Glazecalc yana nuna kalmomin haɗari kamar yadda bayanin laburaren ya ba da su. Wannan ba cikakken kimanta haɗari ba ne, don haka ku karanta takardar bayanan aminci daga mai sayar muku. Kafin ku taɓa kowane kayan glaze, ku karanta Haɗawa cikin aminci da iska mai kyau da Kada ka sa wa iyalinka guba.

Yi amfani da shi a tsarin glaze

Ƙara Longquan Zijin Soil, Gaojitou cikin tsarin glaze a kalkuletan Glazecalc don ganin abin da yake yi wa UMF na glaze.

Buɗe kalkuletan tsarin glazeDuk kayan aiki na asali

Buɗe asusu kyauta