Ihe ọ bụ

Ụdị
Ụrọ
Ọnọdụ
Nke oge gara aga
Formula
SiO₂ 66.93%, Al₂O₃ 18.01%, CaO 1.23%, MgO 0.51%, K₂O 5.23%, Na₂O 0.45%, Fe₂O₃ 3.11%, TiO₂ 0.45%, MnO 0.08%, LOI 4.47%
A na-akpọkwa ya
Gaojitou Zijin soil, Zijin soil, 紫金土
Ihe ndị yiri ya
Redart
Ebe o si
He Z., Zhang M., Zhang H., 'Data-driven research on chemical features of Jingdezhen and Longquan celadon by energy dispersive X-ray fluorescence', arXiv:1511.07825 (2015), Table 6 (2015)

Akụkọ ihe mere eme: ụrọ obodo nwere ọtụtụ iron (紫金土) site n'obodo nta Gaojitou na Dayao, dị nso na kiln Longquan na China, nke a na-agbakwunye n'ụrọ Longquan maka iron na alumina ya; a naghị ere ya na mpụga China. Nke a bụ otu nyocha, nke akwụkwọ ahụ hotara site na nnyocha China gara aga. Otu e si gwuo ya ma kwadebe ya adịghị n'isi mmalite ahụ.

Nyocha oxide na unity formula

Glazecalc nwere nyocha Longquan Zijin Soil, Gaojitou dịka pasent ịdị arọ nke ihe ahụ a na-agbabeghị ọkụ. Ntinye unity bụ moles nke oxide ọ bụla n'ọnụ ọgụgụ Longquan Zijin Soil, Gaojitou nke nwere 1.0 mole nke flux; otu a ka Glazecalc si agbakwunye ya n'unity formula nke usoro.

Oxide dị na Longquan Zijin Soil, Gaojitou
Oxide Ịdị arọ % Ntinye unity
SiO₂66.9311.309
Al₂O₃18.011.793
CaO1.230.223
MgO0.510.128
K₂O5.230.564
Na₂O0.450.074
Fe₂O₃3.110.198
TiO₂0.450.057
MnO0.080.011
Ịdị arọ nhata (equivalent weight)
1015.24
Ịdị arọ mgbe a gbara ọkụ
969.85
Loss on ignition (LOI)
4.47%

Ịdị arọ nhata bụ grams nke Longquan Zijin Soil, Gaojitou nke nwere 1.0 mole nke flux. Ịdị arọ mgbe a gbara ọkụ bụ ihe fọdụrụ na ya mgbe a gbachara ọkụ.

Ihe ize ndụ na nchekwa

Ihe ize ndụ: O nwere crystalline silica; zere iku uzuzu ya.

Glazecalc na-egosi okwu ihe ize ndụ dịka ndekọ ọbá akwụkwọ si dee ya. Ọ bụghị nyocha ihe ize ndụ zuru ezu, ya mere gụọ mpempe data nchekwa site n'aka onye na-ere gị ya. Tupu i metụ ihe glaze ọ bụla, gụọ Ịgwakọta n'enweghị ihe ize ndụ na ikuku dị ọcha na Enyela ezinụlọ gị nsí.

Jiri ya n'usoro

Tinye Longquan Zijin Soil, Gaojitou n'usoro na Glazecalc calculator ka ị hụ ihe ọ na-eme unity formula nke glaze.

Mepee calculator usoroIhe niile a na-ejikarị