Longquan Zijin Soil, Gaojitou
Okokwakha okujwayelekile kumtapo we-Glazecalc: ukuhlaziywa kwako kwe-oxide, isabelo se-unity nezingozi.
Kuyini
- Uhlobo
- Ubumba
- Isimo
- Okomlando
- I-formula
- SiO₂ 66.93%, Al₂O₃ 18.01%, CaO 1.23%, MgO 0.51%, K₂O 5.23%, Na₂O 0.45%, Fe₂O₃ 3.11%, TiO₂ 0.45%, MnO 0.08%, LOI 4.47%
- Kubizwa nangokuthi
- Gaojitou Zijin soil, Zijin soil, 紫金土
- Okokwakha okufanayo
- Redart
- Umthombo
- He Z., Zhang M., Zhang H., 'Data-driven research on chemical features of Jingdezhen and Longquan celadon by energy dispersive X-ray fluorescence', arXiv:1511.07825 (2015), Table 6 (2015)
Okomlando: ubumba lwendawo olunensimbi eningi (紫金土) oluvela esigodini sase-Gaojitou e-Dayao, eduze kwama-kiln ase-Longquan eShayina, olwengezwa kubumba lwase-Longquan ngenxa yensimbi ne-alumina yalo; aluthengiswa ngaphandle kweShayina. Lokhu ukuhlaziywa okukodwa, okucashunwa yiphepha ezifundweni zangaphambili zaseShayina. Ukuthi lwambiwa futhi lwalungiswa kanjani akukho emthonjeni.
Ukuhlaziywa kwe-oxide ne-unity formula
I-Glazecalc inokuhlaziywa kwe-Longquan Zijin Soil, Gaojitou njengephesenti lesisindo sokokwakha okuluhlaza. Isabelo se-unity singama-mole e-oxide ngayinye enanini le-Longquan Zijin Soil, Gaojitou eliqukethe i-mole engu-1.0 ye-flux, okuyindlela i-Glazecalc eyengeza ngayo ku-unity formula yeresiphi.
| I-oxide | Isisindo % | Isabelo se-unity |
|---|---|---|
| SiO₂ | 66.93 | 11.309 |
| Al₂O₃ | 18.01 | 1.793 |
| CaO | 1.23 | 0.223 |
| MgO | 0.51 | 0.128 |
| K₂O | 5.23 | 0.564 |
| Na₂O | 0.45 | 0.074 |
| Fe₂O₃ | 3.11 | 0.198 |
| TiO₂ | 0.45 | 0.057 |
| MnO | 0.08 | 0.011 |
- Isisindo esilinganayo
- 1015.24
- Isisindo esishisiwe
- 969.85
- I-loss on ignition
- 4.47%
Isisindo esilinganayo singamagremu e-Longquan Zijin Soil, Gaojitou aqukethe i-mole engu-1.0 ye-flux. Isisindo esishisiwe yilokho okusalayo kulokho ngemva kokushisa.
Izingozi nokuphepha
Izingozi: Kuqukethe i-silica eyikristalu; gwema ukuhogela uthuli.
Kusebenzise eresiphini
Engeza i-Longquan Zijin Soil, Gaojitou eresiphini ku-calculator ye-Glazecalc ukuze ubone ukuthi yenzani ku-unity formula ye-glaze.