Waxa uu yahay

Nooca
Dhoobooyin
Xaaladda
Taariikhi
Qaacidada
SiO₂ 66.93%, Al₂O₃ 18.01%, CaO 1.23%, MgO 0.51%, K₂O 5.23%, Na₂O 0.45%, Fe₂O₃ 3.11%, TiO₂ 0.45%, MnO 0.08%, LOI 4.47%
Sidoo kale loo yaqaan
Gaojitou Zijin soil, Zijin soil, 紫金土
Walxo la mid ah
Redart
Isha
He Z., Zhang M., Zhang H., 'Data-driven research on chemical features of Jingdezhen and Longquan celadon by energy dispersive X-ray fluorescence', arXiv:1511.07825 (2015), Table 6 (2015)

Taariikhi: dhoobo deegaan ah oo bir badan leh (紫金土) oo ka timid tuulada Gaojitou ee Dayao, una dhow kiln-yada Longquan ee Shiinaha, oo lagu daro dhoobada Longquan biraheeda iyo alumina-deeda darteed; lagama iibiyo Shiinaha dibaddiisa. Kani waa hal falanqayn, oo warqaddu ka soo xigatay daraasado Shiinees ah oo hore. Sida loo qoday loona diyaariyey kuma jiro isha.

Falanqaynta oksaydhka iyo UMF (unity molecular formula)

Glazecalc wuxuu hayaa falanqaynta walaxda Longquan Zijin Soil, Gaojitou oo ah boqolkiiba miisaanka walaxda ceeriin. Qaybta UMF waa moles-ka oksaydh kasta ee ku jira xaddiga walaxda Longquan Zijin Soil, Gaojitou ee haysta 1.0 mole oo flux ah, taasina waa sida Glazecalc ugu daro UMF-ta habka.

Oksaydhyada ku jira walaxda Longquan Zijin Soil, Gaojitou
Oksaydh Miisaan % Qaybta UMF
SiO₂66.9311.309
Al₂O₃18.011.793
CaO1.230.223
MgO0.510.128
K₂O5.230.564
Na₂O0.450.074
Fe₂O₃3.110.198
TiO₂0.450.057
MnO0.080.011
Miisaanka u dhigma (equivalent weight)
1015.24
Miisaanka kaddib gubidda
969.85
LOI (lumista gubidda)
4.47%

Miisaanka u dhigma waa garaamada walaxda Longquan Zijin Soil, Gaojitou ee haysta 1.0 mole oo flux ah. Miisaanka kaddib gubidda waa inta ka hadha kaddib gubidda.

Khataraha iyo badbaadada

Khataraha: Waxaa ku jira silica kiristaal ah; iska ilaali neefsashada boodhka.

Glazecalc wuxuu muujiyaa qoraalka khatarta sida diiwaanka maktabaddu u bixiyo. Ma aha qiimayn khatar oo dhammaystiran, sidaas darteed akhri warqadda xogta badbaadada (SDS) ee alaab-qeybiyahaaga. Ka hor intaadan taaban walax glaze kasta, akhri Isku-darka ammaanka ah iyo hawo-wareejinta iyo Ha sumayn qoyskaaga.

Ku isticmaal hab

Ku dar walaxda Longquan Zijin Soil, Gaojitou hab ku jira xisaabiyaha Glazecalc si aad u aragto waxa ay ku samayso UMF-ta glaze-ka.

Fur xisaabiyaha habkaDhammaan walxaha caadiga ah

Samee akoon bilaash ah