Tsushima Feldspar (対馬長石)
Kayan aiki na asali a laburaren Glazecalc: binciken oxide ɗinsa, gudummawar UMF da haɗarinsa.
Mene ne shi
- Nau’i
- Feldspar da duwatsu
- Tsarin sinadarai
- SiO₂ 79.17%, Al₂O₃ 12.07%, Fe₂O₃ 0.06%, TiO₂ 0.1%, CaO 0.67%, MgO 0.2%, Na₂O 6.38%, K₂O 0.41%, LOI 0.88%
- Ana kuma kiransa
- 対馬長石, 対州長石, Taishu feldspar, Tsushima feldspar
- Ana sayar da shi a
- JP
- Tushe
- 佐賀県陶磁器原料株式会社 (Arita): 釉薬原料の化学分析表, the supplier's typical analysis of what it sells (undated; read 2026-11-04)
Nazari na yau da kullum daga mai sayarwa ɗaya a Arita: kwatanta shi da na mai sayar muku. Feldspar na soda mai quartz mai yawa a ware, kusan SiO₂ 79% kuma kusan babu potash, ba tsantsar feldspar ba. Kada ku musanya shi da feldspar na soda ko na potash nauyi da nauyi.
Binciken oxide da UMF
Glazecalc yana da binciken Tsushima Feldspar (対馬長石) a matsayin kashi bisa nauyi na ɗanyen kayan. Gudummawar UMF ita ce mole na kowane oxide a cikin adadin Tsushima Feldspar (対馬長石) da ke ɗauke da mole 1.0 na flux, kuma haka Glazecalc ke ƙara shi cikin UMF (unity molecular formula) na tsarin glaze.
| Oxide | Kashi bisa nauyi % | Gudummawar UMF |
|---|---|---|
| SiO₂ | 79.17 | 10.609 |
| Al₂O₃ | 12.07 | 0.953 |
| Fe₂O₃ | 0.06 | 0.003 |
| TiO₂ | 0.1 | 0.010 |
| CaO | 0.67 | 0.096 |
| MgO | 0.2 | 0.040 |
| Na₂O | 6.38 | 0.829 |
| K₂O | 0.41 | 0.035 |
- Nauyin daidai (equivalent weight)
- 805.15
- Nauyi bayan gasa
- 798.06
- LOI (raguwar nauyi a wuta)
- 0.88%
Nauyin daidai shi ne giram na Tsushima Feldspar (対馬長石) da ke ɗauke da mole 1.0 na flux. Nauyi bayan gasa shi ne abin da ya rage daga wannan bayan gasa.
Haɗari da tsaro
Haɗari: Yana ƙunshe da crystalline silica; ku guji shaƙar ƙurar.
Yi amfani da shi a tsarin glaze
Ƙara Tsushima Feldspar (対馬長石) cikin tsarin glaze a kalkuletan Glazecalc don ganin abin da yake yi wa UMF na glaze.