Ihe ọ bụ

Ụdị
Feldspar na nkume
Formula
SiO₂ 79.17%, Al₂O₃ 12.07%, Fe₂O₃ 0.06%, TiO₂ 0.1%, CaO 0.67%, MgO 0.2%, Na₂O 6.38%, K₂O 0.41%, LOI 0.88%
A na-akpọkwa ya
対馬長石, 対州長石, Taishu feldspar, Tsushima feldspar
A na-ere ya na
JP
Ebe o si
佐賀県陶磁器原料株式会社 (Arita): 釉薬原料の化学分析表, the supplier's typical analysis of what it sells (undated; read 2026-11-04)

Nyocha a na-ahụkarị site n'aka otu onye na-ere ahịa na Arita: tụnyere ya na nke onye na-ere gị. Feldspar soda nwere ọtụtụ quartz nọ onwe ya, ihe dị ka SiO₂ 79% na fọrọ nke nta ka ọ ghara inwe potash, ọ bụghị feldspar dị ọcha. Ejila ya dochie feldspar soda ma ọ bụ nke potash ịdị arọ maka ịdị arọ.

Nyocha oxide na unity formula

Glazecalc nwere nyocha Tsushima Feldspar (対馬長石) dịka pasent ịdị arọ nke ihe ahụ a na-agbabeghị ọkụ. Ntinye unity bụ moles nke oxide ọ bụla n'ọnụ ọgụgụ Tsushima Feldspar (対馬長石) nke nwere 1.0 mole nke flux; otu a ka Glazecalc si agbakwunye ya n'unity formula nke usoro.

Oxide dị na Tsushima Feldspar (対馬長石)
Oxide Ịdị arọ % Ntinye unity
SiO₂79.1710.609
Al₂O₃12.070.953
Fe₂O₃0.060.003
TiO₂0.10.010
CaO0.670.096
MgO0.20.040
Na₂O6.380.829
K₂O0.410.035
Ịdị arọ nhata (equivalent weight)
805.15
Ịdị arọ mgbe a gbara ọkụ
798.06
Loss on ignition (LOI)
0.88%

Ịdị arọ nhata bụ grams nke Tsushima Feldspar (対馬長石) nke nwere 1.0 mole nke flux. Ịdị arọ mgbe a gbara ọkụ bụ ihe fọdụrụ na ya mgbe a gbachara ọkụ.

Ihe ize ndụ na nchekwa

Ihe ize ndụ: O nwere crystalline silica; zere iku uzuzu ya.

Glazecalc na-egosi okwu ihe ize ndụ dịka ndekọ ọbá akwụkwọ si dee ya. Ọ bụghị nyocha ihe ize ndụ zuru ezu, ya mere gụọ mpempe data nchekwa site n'aka onye na-ere gị ya. Tupu i metụ ihe glaze ọ bụla, gụọ Ịgwakọta n'enweghị ihe ize ndụ na ikuku dị ọcha na Enyela ezinụlọ gị nsí.

Jiri ya n'usoro

Tinye Tsushima Feldspar (対馬長石) n'usoro na Glazecalc calculator ka ị hụ ihe ọ na-eme unity formula nke glaze.

Mepee calculator usoroIhe niile a na-ejikarị

Mepụta akaụntụ n'efu