Tsushima Feldspar (対馬長石)
Walax caadi ah oo ku jirta maktabadda Glazecalc: falanqaynta oksaydhka, qaybta UMF iyo khataraha.
Waxa uu yahay
- Nooca
- Feldspar iyo dhagxaan
- Qaacidada
- SiO₂ 79.17%, Al₂O₃ 12.07%, Fe₂O₃ 0.06%, TiO₂ 0.1%, CaO 0.67%, MgO 0.2%, Na₂O 6.38%, K₂O 0.41%, LOI 0.88%
- Sidoo kale loo yaqaan
- 対馬長石, 対州長石, Taishu feldspar, Tsushima feldspar
- Waxaa lagu iibiyaa
- JP
- Isha
- 佐賀県陶磁器原料株式会社 (Arita): 釉薬原料の化学分析表, the supplier's typical analysis of what it sells (undated; read 2026-11-04)
Falanqayn caadi ah oo ka timid hal iibiye oo Arita ku sugan: barbardhig tan iibiyahaaga. Feldspar soda ah oo leh quartz xor ah oo badan, qiyaastii 79% SiO₂ oo ku dhowaad aan potash lahayn, ma aha feldspar saafi ah. Ha ku beddelin feldspar soda ama potash ah miisaan miisaan.
Falanqaynta oksaydhka iyo UMF (unity molecular formula)
Glazecalc wuxuu hayaa falanqaynta walaxda Tsushima Feldspar (対馬長石) oo ah boqolkiiba miisaanka walaxda ceeriin. Qaybta UMF waa moles-ka oksaydh kasta ee ku jira xaddiga walaxda Tsushima Feldspar (対馬長石) ee haysta 1.0 mole oo flux ah, taasina waa sida Glazecalc ugu daro UMF-ta habka.
| Oksaydh | Miisaan % | Qaybta UMF |
|---|---|---|
| SiO₂ | 79.17 | 10.609 |
| Al₂O₃ | 12.07 | 0.953 |
| Fe₂O₃ | 0.06 | 0.003 |
| TiO₂ | 0.1 | 0.010 |
| CaO | 0.67 | 0.096 |
| MgO | 0.2 | 0.040 |
| Na₂O | 6.38 | 0.829 |
| K₂O | 0.41 | 0.035 |
- Miisaanka u dhigma (equivalent weight)
- 805.15
- Miisaanka kaddib gubidda
- 798.06
- LOI (lumista gubidda)
- 0.88%
Miisaanka u dhigma waa garaamada walaxda Tsushima Feldspar (対馬長石) ee haysta 1.0 mole oo flux ah. Miisaanka kaddib gubidda waa inta ka hadha kaddib gubidda.
Khataraha iyo badbaadada
Khataraha: Waxaa ku jira silica kiristaal ah; iska ilaali neefsashada boodhka.
Ku isticmaal hab
Ku dar walaxda Tsushima Feldspar (対馬長石) hab ku jira xisaabiyaha Glazecalc si aad u aragto waxa ay ku samayso UMF-ta glaze-ka.