Kuyini

Uhlobo
Ama-feldspar namatshe
I-formula
SiO₂ 79.17%, Al₂O₃ 12.07%, Fe₂O₃ 0.06%, TiO₂ 0.1%, CaO 0.67%, MgO 0.2%, Na₂O 6.38%, K₂O 0.41%, LOI 0.88%
Kubizwa nangokuthi
対馬長石, 対州長石, Taishu feldspar, Tsushima feldspar
Kuthengiswa e
JP
Umthombo
佐賀県陶磁器原料株式会社 (Arita): 釉薬原料の化学分析表, the supplier's typical analysis of what it sells (undated; read 2026-11-04)

Ukuhlaziywa okujwayelekile okuvela kumphakeli oyedwa e-Arita: kuqhathanise nokomphakeli wakho. I-feldspar ye-soda ene-quartz ekhululekile eningi, cishe u-79% SiO₂ futhi icishe ingabi ne-potash, hhayi i-feldspar emsulwa. Ungayishintshi nge-feldspar ye-soda noma ye-potash isisindo ngesisindo.

Ukuhlaziywa kwe-oxide ne-unity formula

I-Glazecalc inokuhlaziywa kwe-Tsushima Feldspar (対馬長石) njengephesenti lesisindo sokokwakha okuluhlaza. Isabelo se-unity singama-mole e-oxide ngayinye enanini le-Tsushima Feldspar (対馬長石) eliqukethe i-mole engu-1.0 ye-flux, okuyindlela i-Glazecalc eyengeza ngayo ku-unity formula yeresiphi.

Ama-oxide aku-Tsushima Feldspar (対馬長石)
I-oxide Isisindo % Isabelo se-unity
SiO₂79.1710.609
Al₂O₃12.070.953
Fe₂O₃0.060.003
TiO₂0.10.010
CaO0.670.096
MgO0.20.040
Na₂O6.380.829
K₂O0.410.035
Isisindo esilinganayo
805.15
Isisindo esishisiwe
798.06
I-loss on ignition
0.88%

Isisindo esilinganayo singamagremu e-Tsushima Feldspar (対馬長石) aqukethe i-mole engu-1.0 ye-flux. Isisindo esishisiwe yilokho okusalayo kulokho ngemva kokushisa.

Izingozi nokuphepha

Izingozi: Kuqukethe i-silica eyikristalu; gwema ukuhogela uthuli.

I-Glazecalc ibonisa amagama engozi njengoba irekhodi lomtapo liwanikeza. Akukona ukuhlolwa okugcwele kwengozi, ngakho funda ishidi lemininingwane yokuphepha elivela kumphakeli wakho. Ngaphambi kokuthi uthinte noma yikuphi okokwakha kwe-glaze, funda Ukuxuba ngokuphepha nomoya ohlanzekile futhi Ungawadliseli ushevu umndeni wakho.

Kusebenzise eresiphini

Engeza i-Tsushima Feldspar (対馬長石) eresiphini ku-calculator ye-Glazecalc ukuze ubone ukuthi yenzani ku-unity formula ye-glaze.

Vula i-calculator yeresiphiKonke okokwakha okujwayelekile

Vula i-akhawunti yamahhala