Mene ne shi

Nau’i
Flux (masu narkarwa)
Tsarin sinadarai
SiO₂ 17.59%, Al₂O₃ 3.13%, Fe₂O₃ 0.31%, CaO 37.09%, MgO 5.25%, Na₂O 0.06%, K₂O 0.17%, LOI 36.4%
Ana kuma kiransa
合成柞灰, 合成イス灰, gōsei isubai
Ana sayar da shi a
JP
Tushe
佐賀県陶磁器原料株式会社 (Arita): 釉薬原料の化学分析表, the supplier's typical analysis of what it sells (undated; read 2026-11-04)

Nazari na yau da kullum daga mai sayarwa ɗaya a Arita: kwatanta shi da na mai sayar muku. Madadin da aka ƙera (synthetic) na 柞灰 (tokar isu), tokar itace ta glaze na Japan; ba toka ta gaske ba ce, wadda take bambanta sosai. Adadin mai sayarwar ya kai 96.48%, don haka 3.52% da suka bari ana ƙirga shi a nan a matsayin abin da ya ɓace a gasa, tare da LOI ɗinsa na 32.88%.

Binciken oxide da UMF

Glazecalc yana da binciken Synthetic Isu Ash (合成柞灰) a matsayin kashi bisa nauyi na ɗanyen kayan. Gudummawar UMF ita ce mole na kowane oxide a cikin adadin Synthetic Isu Ash (合成柞灰) da ke ɗauke da mole 1.0 na flux, kuma haka Glazecalc ke ƙara shi cikin UMF (unity molecular formula) na tsarin glaze.

Oxide a cikin Synthetic Isu Ash (合成柞灰)
Oxide Kashi bisa nauyi % Gudummawar UMF
SiO₂17.590.369
Al₂O₃3.130.039
Fe₂O₃0.310.002
CaO37.090.833
MgO5.250.164
Na₂O0.060.001
K₂O0.170.002
Nauyin daidai (equivalent weight)
125.87
Nauyi bayan gasa
80.06
LOI (raguwar nauyi a wuta)
36.4%

Nauyin daidai shi ne giram na Synthetic Isu Ash (合成柞灰) da ke ɗauke da mole 1.0 na flux. Nauyi bayan gasa shi ne abin da ya rage daga wannan bayan gasa.

Haɗari da tsaro

Haɗari: Ku guji shaƙar ƙurar.

Glazecalc yana nuna kalmomin haɗari kamar yadda bayanin laburaren ya ba da su. Wannan ba cikakken kimanta haɗari ba ne, don haka ku karanta takardar bayanan aminci daga mai sayar muku. Kafin ku taɓa kowane kayan glaze, ku karanta Haɗawa cikin aminci da iska mai kyau da Kada ka sa wa iyalinka guba.

Yi amfani da shi a tsarin glaze

Ƙara Synthetic Isu Ash (合成柞灰) cikin tsarin glaze a kalkuletan Glazecalc don ganin abin da yake yi wa UMF na glaze.

Buɗe kalkuletan tsarin glazeDuk kayan aiki na asali