Kuyini

Uhlobo
Ama-flux
I-formula
SiO₂ 17.59%, Al₂O₃ 3.13%, Fe₂O₃ 0.31%, CaO 37.09%, MgO 5.25%, Na₂O 0.06%, K₂O 0.17%, LOI 36.4%
Kubizwa nangokuthi
合成柞灰, 合成イス灰, gōsei isubai
Kuthengiswa e
JP
Umthombo
佐賀県陶磁器原料株式会社 (Arita): 釉薬原料の化学分析表, the supplier's typical analysis of what it sells (undated; read 2026-11-04)

Ukuhlaziywa okujwayelekile okuvela kumphakeli oyedwa e-Arita: kuqhathanise nokomphakeli wakho. Okufakwa esikhundleni okwenziwe (synthetic) kwe-柞灰 (umlotha we-isu), umlotha wezinkuni wama-glaze aseJapan; akuwona umlotha wangempela, oshintsha kakhulu. Izibalo zomphakeli zihlangana zibe ngu-96.48%, ngakho u-3.52% abawushiyayo ubalwa lapha njengolahleka ekushiseni, ne-LOI yawo engu-32.88%.

Ukuhlaziywa kwe-oxide ne-unity formula

I-Glazecalc inokuhlaziywa kwe-Synthetic Isu Ash (合成柞灰) njengephesenti lesisindo sokokwakha okuluhlaza. Isabelo se-unity singama-mole e-oxide ngayinye enanini le-Synthetic Isu Ash (合成柞灰) eliqukethe i-mole engu-1.0 ye-flux, okuyindlela i-Glazecalc eyengeza ngayo ku-unity formula yeresiphi.

Ama-oxide aku-Synthetic Isu Ash (合成柞灰)
I-oxide Isisindo % Isabelo se-unity
SiO₂17.590.369
Al₂O₃3.130.039
Fe₂O₃0.310.002
CaO37.090.833
MgO5.250.164
Na₂O0.060.001
K₂O0.170.002
Isisindo esilinganayo
125.87
Isisindo esishisiwe
80.06
I-loss on ignition
36.4%

Isisindo esilinganayo singamagremu e-Synthetic Isu Ash (合成柞灰) aqukethe i-mole engu-1.0 ye-flux. Isisindo esishisiwe yilokho okusalayo kulokho ngemva kokushisa.

Izingozi nokuphepha

Izingozi: Gwema ukuhogela uthuli.

I-Glazecalc ibonisa amagama engozi njengoba irekhodi lomtapo liwanikeza. Akukona ukuhlolwa okugcwele kwengozi, ngakho funda ishidi lemininingwane yokuphepha elivela kumphakeli wakho. Ngaphambi kokuthi uthinte noma yikuphi okokwakha kwe-glaze, funda Ukuxuba ngokuphepha nomoya ohlanzekile futhi Ungawadliseli ushevu umndeni wakho.

Kusebenzise eresiphini

Engeza i-Synthetic Isu Ash (合成柞灰) eresiphini ku-calculator ye-Glazecalc ukuze ubone ukuthi yenzani ku-unity formula ye-glaze.

Vula i-calculator yeresiphiKonke okokwakha okujwayelekile

Vula i-akhawunti yamahhala