Waxa uu yahay
- Nooca
- Flux-yo
- Qaacidada
- SiO₂ 17.59%, Al₂O₃ 3.13%, Fe₂O₃ 0.31%, CaO 37.09%, MgO 5.25%, Na₂O 0.06%, K₂O 0.17%, LOI 36.4%
- Sidoo kale loo yaqaan
- 合成柞灰, 合成イス灰, gōsei isubai
- Waxaa lagu iibiyaa
- JP
- Isha
- 佐賀県陶磁器原料株式会社 (Arita): 釉薬原料の化学分析表, the supplier's typical analysis of what it sells (undated; read 2026-11-04)
Falanqayn caadi ah oo ka timid hal iibiye oo Arita ku sugan: barbardhig tan iibiyahaaga. Beddel la sameeyey (synthetic) oo loogu talagalay 柞灰 (dambaska isu), dambas qoryo ee glaze-yada Japan; ma aha dambas dhab ah, kaas oo aad u kala duwan. Tirooyinka iibiyuhu waxay isku gaarayaan 96.48%, sidaa darteed 3.52% ay ka tageen halkan waxaa lagu tiriyaa wax gubidda ku lumay, oo leh LOI-giisa 32.88%.
Falanqaynta oksaydhka iyo UMF (unity molecular formula)
Glazecalc wuxuu hayaa falanqaynta walaxda Synthetic Isu Ash (合成柞灰) oo ah boqolkiiba miisaanka walaxda ceeriin. Qaybta UMF waa moles-ka oksaydh kasta ee ku jira xaddiga walaxda Synthetic Isu Ash (合成柞灰) ee haysta 1.0 mole oo flux ah, taasina waa sida Glazecalc ugu daro UMF-ta habka.
| Oksaydh | Miisaan % | Qaybta UMF |
|---|---|---|
| SiO₂ | 17.59 | 0.369 |
| Al₂O₃ | 3.13 | 0.039 |
| Fe₂O₃ | 0.31 | 0.002 |
| CaO | 37.09 | 0.833 |
| MgO | 5.25 | 0.164 |
| Na₂O | 0.06 | 0.001 |
| K₂O | 0.17 | 0.002 |
- Miisaanka u dhigma (equivalent weight)
- 125.87
- Miisaanka kaddib gubidda
- 80.06
- LOI (lumista gubidda)
- 36.4%
Miisaanka u dhigma waa garaamada walaxda Synthetic Isu Ash (合成柞灰) ee haysta 1.0 mole oo flux ah. Miisaanka kaddib gubidda waa inta ka hadha kaddib gubidda.
Khataraha iyo badbaadada
Khataraha: Ka fogow neefsashada boodhka.
Ku isticmaal hab
Ku dar walaxda Synthetic Isu Ash (合成柞灰) hab ku jira xisaabiyaha Glazecalc si aad u aragto waxa ay ku samayso UMF-ta glaze-ka.