Korean Kaolin (韓国カオリン)
Kayan aiki na asali a laburaren Glazecalc: binciken oxide ɗinsa, gudummawar UMF da haɗarinsa.
Mene ne shi
- Nau’i
- Yumɓu
- Tsarin sinadarai
- SiO₂ 47.4%, Al₂O₃ 35.26%, Fe₂O₃ 1.22%, TiO₂ 0.18%, CaO 1.17%, MgO 0.44%, Na₂O 0.75%, K₂O 0.84%, LOI 12.67%
- Ana kuma kiransa
- 韓国カオリン, Korean kaolin
- Ana sayar da shi a
- JP
- Tushe
- 佐賀県陶磁器原料株式会社 (Arita): 釉薬原料の化学分析表, the supplier's typical analysis of what it sells (undated; read 2026-11-04)
Nazari na yau da kullum daga mai sayarwa ɗaya a Arita: kwatanta shi da na mai sayar muku. Kaolin daga Korea, da ake sayarwa a Japan. Da Fe₂O₃ 1.22% yana da ƙarfe fiye da kaolin masu ƙarancin ƙarfe, don haka ba ya yin fari sosai idan an gasa.
Binciken oxide da UMF
Glazecalc yana da binciken Korean Kaolin (韓国カオリン) a matsayin kashi bisa nauyi na ɗanyen kayan. Gudummawar UMF ita ce mole na kowane oxide a cikin adadin Korean Kaolin (韓国カオリン) da ke ɗauke da mole 1.0 na flux, kuma haka Glazecalc ke ƙara shi cikin UMF (unity molecular formula) na tsarin glaze.
| Oxide | Kashi bisa nauyi % | Gudummawar UMF |
|---|---|---|
| SiO₂ | 47.4 | 14.942 |
| Al₂O₃ | 35.26 | 6.550 |
| Fe₂O₃ | 1.22 | 0.145 |
| TiO₂ | 0.18 | 0.043 |
| CaO | 1.17 | 0.395 |
| MgO | 0.44 | 0.207 |
| Na₂O | 0.75 | 0.229 |
| K₂O | 0.84 | 0.169 |
- Nauyin daidai (equivalent weight)
- 1893.95
- Nauyi bayan gasa
- 1653.99
- LOI (raguwar nauyi a wuta)
- 12.67%
Nauyin daidai shi ne giram na Korean Kaolin (韓国カオリン) da ke ɗauke da mole 1.0 na flux. Nauyi bayan gasa shi ne abin da ya rage daga wannan bayan gasa.
Haɗari da tsaro
Haɗari: Ƙurar kaolin; tana iya ƙunsar ɗan crystalline silica (quartz). Ku guji shaƙar ƙurar.
Yi amfani da shi a tsarin glaze
Ƙara Korean Kaolin (韓国カオリン) cikin tsarin glaze a kalkuletan Glazecalc don ganin abin da yake yi wa UMF na glaze.