Kuyini

Uhlobo
Ubumba
I-formula
SiO₂ 47.4%, Al₂O₃ 35.26%, Fe₂O₃ 1.22%, TiO₂ 0.18%, CaO 1.17%, MgO 0.44%, Na₂O 0.75%, K₂O 0.84%, LOI 12.67%
Kubizwa nangokuthi
韓国カオリン, Korean kaolin
Kuthengiswa e
JP
Umthombo
佐賀県陶磁器原料株式会社 (Arita): 釉薬原料の化学分析表, the supplier's typical analysis of what it sells (undated; read 2026-11-04)

Ukuhlaziywa okujwayelekile okuvela kumphakeli oyedwa e-Arita: kuqhathanise nokomphakeli wakho. I-kaolin evela eKorea, ethengiswa eJapan. Ngo-1.22% Fe₂O₃ inensimbi eningi kunama-kaolin anensimbi encane, ngakho ayibi mhlophe kangako uma ishisiwe.

Ukuhlaziywa kwe-oxide ne-unity formula

I-Glazecalc inokuhlaziywa kwe-Korean Kaolin (韓国カオリン) njengephesenti lesisindo sokokwakha okuluhlaza. Isabelo se-unity singama-mole e-oxide ngayinye enanini le-Korean Kaolin (韓国カオリン) eliqukethe i-mole engu-1.0 ye-flux, okuyindlela i-Glazecalc eyengeza ngayo ku-unity formula yeresiphi.

Ama-oxide aku-Korean Kaolin (韓国カオリン)
I-oxide Isisindo % Isabelo se-unity
SiO₂47.414.942
Al₂O₃35.266.550
Fe₂O₃1.220.145
TiO₂0.180.043
CaO1.170.395
MgO0.440.207
Na₂O0.750.229
K₂O0.840.169
Isisindo esilinganayo
1893.95
Isisindo esishisiwe
1653.99
I-loss on ignition
12.67%

Isisindo esilinganayo singamagremu e-Korean Kaolin (韓国カオリン) aqukethe i-mole engu-1.0 ye-flux. Isisindo esishisiwe yilokho okusalayo kulokho ngemva kokushisa.

Izingozi nokuphepha

Izingozi: Uthuli lwe-kaolin; lungaqukatha i-silica eyikristalu encane (i-quartz). Gwema ukuhogela uthuli.

I-Glazecalc ibonisa amagama engozi njengoba irekhodi lomtapo liwanikeza. Akukona ukuhlolwa okugcwele kwengozi, ngakho funda ishidi lemininingwane yokuphepha elivela kumphakeli wakho. Ngaphambi kokuthi uthinte noma yikuphi okokwakha kwe-glaze, funda Ukuxuba ngokuphepha nomoya ohlanzekile futhi Ungawadliseli ushevu umndeni wakho.

Kusebenzise eresiphini

Engeza i-Korean Kaolin (韓国カオリン) eresiphini ku-calculator ye-Glazecalc ukuze ubone ukuthi yenzani ku-unity formula ye-glaze.

Vula i-calculator yeresiphiKonke okokwakha okujwayelekile

Vula i-akhawunti yamahhala