Korean Kaolin (韓国カオリン)
Walax caadi ah oo ku jirta maktabadda Glazecalc: falanqaynta oksaydhka, qaybta UMF iyo khataraha.
Waxa uu yahay
- Nooca
- Dhoobooyin
- Qaacidada
- SiO₂ 47.4%, Al₂O₃ 35.26%, Fe₂O₃ 1.22%, TiO₂ 0.18%, CaO 1.17%, MgO 0.44%, Na₂O 0.75%, K₂O 0.84%, LOI 12.67%
- Sidoo kale loo yaqaan
- 韓国カオリン, Korean kaolin
- Waxaa lagu iibiyaa
- JP
- Isha
- 佐賀県陶磁器原料株式会社 (Arita): 釉薬原料の化学分析表, the supplier's typical analysis of what it sells (undated; read 2026-11-04)
Falanqayn caadi ah oo ka timid hal iibiye oo Arita ku sugan: barbardhig tan iibiyahaaga. Kaolin ka timid Kuuriya, oo laga iibiyo Japan. Isagoo leh 1.22% Fe₂O₃ wuxuu leeyahay bir ka badan kaolin-yada birta yar, sidaa darteed marka la gubo aad uma cadaado.
Falanqaynta oksaydhka iyo UMF (unity molecular formula)
Glazecalc wuxuu hayaa falanqaynta walaxda Korean Kaolin (韓国カオリン) oo ah boqolkiiba miisaanka walaxda ceeriin. Qaybta UMF waa moles-ka oksaydh kasta ee ku jira xaddiga walaxda Korean Kaolin (韓国カオリン) ee haysta 1.0 mole oo flux ah, taasina waa sida Glazecalc ugu daro UMF-ta habka.
| Oksaydh | Miisaan % | Qaybta UMF |
|---|---|---|
| SiO₂ | 47.4 | 14.942 |
| Al₂O₃ | 35.26 | 6.550 |
| Fe₂O₃ | 1.22 | 0.145 |
| TiO₂ | 0.18 | 0.043 |
| CaO | 1.17 | 0.395 |
| MgO | 0.44 | 0.207 |
| Na₂O | 0.75 | 0.229 |
| K₂O | 0.84 | 0.169 |
- Miisaanka u dhigma (equivalent weight)
- 1893.95
- Miisaanka kaddib gubidda
- 1653.99
- LOI (lumista gubidda)
- 12.67%
Miisaanka u dhigma waa garaamada walaxda Korean Kaolin (韓国カオリン) ee haysta 1.0 mole oo flux ah. Miisaanka kaddib gubidda waa inta ka hadha kaddib gubidda.
Khataraha iyo badbaadada
Khataraha: Boodh kaolin; waxaa ku jiri kara wax yar oo silica kiristaal ah (quartz). Iska ilaali neefsashada boodhka.
Ku isticmaal hab
Ku dar walaxda Korean Kaolin (韓国カオリン) hab ku jira xisaabiyaha Glazecalc si aad u aragto waxa ay ku samayso UMF-ta glaze-ka.