Feldspar da duwatsu
Matsayi
Na tarihi
Tsarin sinadarai
SiO₂ 73.7%, Al₂O₃ 15.34%, CaO 0.7%, MgO 0.16%, K₂O 4.13%, Na₂O 3.79%, Fe₂O₃ 0.7%, MnO 0.04%, LOI 1.13%
Ana kuma kiransa
Sanbaopeng chinastone, San Bao porcelain stone
Kayan aiki masu kama
H&G Cornwall Stone , Cornish Stone (synthetic substitute) , Cornish Stone, Synthetic (Walker BA280) , Amakusa Pottery Stone (天草陶石)
Tushe
He Z., Zhang M., Zhang H., 'Data-driven research on chemical features of Jingdezhen and Longquan celadon by energy dispersive X-ray fluorescence', arXiv:1511.07825 (2015), Table 6. Second analysis: derekau.net, 'Porcelain Stone Glazes' (2015), quoting 陶瓷艺术釉工艺学 (江西高校出版社) (2015)

Na tarihi: dutsen porcelain (瓷石) daga ƙauyen San Bao kusa da Jingdezhen, China, da aka haƙa a can aka sayar wa masana'antun tukwane a matsayin bulo; ba a sayar da shi a wajen China. Wannan nazari ɗaya ne, wanda takardar ta ɗauko daga binciken China na baya. Wani, daga littafin koyar da glaze na Jiangxi, ya kusan zama ɗaya, da Al₂O₃ 17.64%, K₂O 4.02% da Na₂O 4.68%, kuma dutse daga San Bao yana bambanta tsakanin masu samarwa da kuma daga shekara zuwa shekara.

Binciken oxide da UMF

Glazecalc yana da binciken Jingdezhen Porcelain Stone, Sanbaopeng a matsayin kashi bisa nauyi na ɗanyen kayan. Gudummawar UMF ita ce mole na kowane oxide a cikin adadin Jingdezhen Porcelain Stone, Sanbaopeng da ke ɗauke da mole 1.0 na flux, kuma haka Glazecalc ke ƙara shi cikin UMF (unity molecular formula) na tsarin glaze.

Oxide a cikin Jingdezhen Porcelain Stone, Sanbaopeng
Oxide Kashi bisa nauyi % Gudummawar UMF
SiO₂73.710.053
Al₂O₃15.341.233
CaO0.70.102
MgO0.160.033
K₂O4.130.359
Na₂O3.790.501
Fe₂O₃0.70.036
MnO0.040.005
Nauyin daidai (equivalent weight)
819.59
Nauyi bayan gasa
810.33
LOI (raguwar nauyi a wuta)
1.13%

Nauyin daidai shi ne giram na Jingdezhen Porcelain Stone, Sanbaopeng da ke ɗauke da mole 1.0 na flux. Nauyi bayan gasa shi ne abin da ya rage daga wannan bayan gasa.

Haɗari da tsaro

Haɗari: Yana ƙunshe da crystalline silica; ku guji shaƙar ƙurar.

Glazecalc yana nuna kalmomin haɗari kamar yadda bayanin laburaren ya ba da su. Wannan ba cikakken kimanta haɗari ba ne, don haka ku karanta takardar bayanan aminci daga mai sayar muku. Kafin ku taɓa kowane kayan glaze, ku karanta Haɗawa cikin aminci da iska mai kyau da Kada ka sa wa iyalinka guba.

Yi amfani da shi a tsarin glaze

Ƙara Jingdezhen Porcelain Stone, Sanbaopeng cikin tsarin glaze a kalkuletan Glazecalc don ganin abin da yake yi wa UMF na glaze.

Buɗe kalkuletan tsarin glazeDuk kayan aiki na asali

Buɗe asusu kyauta