Kuyini

Uhlobo
Ama-feldspar namatshe
Isimo
Okomlando
I-formula
SiO₂ 73.7%, Al₂O₃ 15.34%, CaO 0.7%, MgO 0.16%, K₂O 4.13%, Na₂O 3.79%, Fe₂O₃ 0.7%, MnO 0.04%, LOI 1.13%
Kubizwa nangokuthi
Sanbaopeng chinastone, San Bao porcelain stone
Okokwakha okufanayo
H&G Cornwall Stone , Cornish Stone (synthetic substitute) , Cornish Stone, Synthetic (Walker BA280) , Amakusa Pottery Stone (天草陶石)
Umthombo
He Z., Zhang M., Zhang H., 'Data-driven research on chemical features of Jingdezhen and Longquan celadon by energy dispersive X-ray fluorescence', arXiv:1511.07825 (2015), Table 6. Second analysis: derekau.net, 'Porcelain Stone Glazes' (2015), quoting 陶瓷艺术釉工艺学 (江西高校出版社) (2015)

Okomlando: itshe le-porcelain (瓷石) elivela esigodini sase-San Bao eduze kwase-Jingdezhen, eShayina, elamajwa khona futhi lathengiselwa izindawo zokubumba njengezitini; alithengiswa ngaphandle kweShayina. Lokhu ukuhlaziywa okukodwa, okucashunwa yiphepha ezifundweni zangaphambili zaseShayina. Okunye, okuvela encwadini yokufunda nge-glaze yase-Jiangxi, kucishe kufane, kune-17.64% Al₂O₃, 4.02% K₂O no-4.68% Na₂O, futhi itshe lase-San Bao liyahluka phakathi kwabakhiqizi nangonyaka nonyaka.

Ukuhlaziywa kwe-oxide ne-unity formula

I-Glazecalc inokuhlaziywa kwe-Jingdezhen Porcelain Stone, Sanbaopeng njengephesenti lesisindo sokokwakha okuluhlaza. Isabelo se-unity singama-mole e-oxide ngayinye enanini le-Jingdezhen Porcelain Stone, Sanbaopeng eliqukethe i-mole engu-1.0 ye-flux, okuyindlela i-Glazecalc eyengeza ngayo ku-unity formula yeresiphi.

Ama-oxide aku-Jingdezhen Porcelain Stone, Sanbaopeng
I-oxide Isisindo % Isabelo se-unity
SiO₂73.710.053
Al₂O₃15.341.233
CaO0.70.102
MgO0.160.033
K₂O4.130.359
Na₂O3.790.501
Fe₂O₃0.70.036
MnO0.040.005
Isisindo esilinganayo
819.59
Isisindo esishisiwe
810.33
I-loss on ignition
1.13%

Isisindo esilinganayo singamagremu e-Jingdezhen Porcelain Stone, Sanbaopeng aqukethe i-mole engu-1.0 ye-flux. Isisindo esishisiwe yilokho okusalayo kulokho ngemva kokushisa.

Izingozi nokuphepha

Izingozi: Kuqukethe i-silica eyikristalu; gwema ukuhogela uthuli.

I-Glazecalc ibonisa amagama engozi njengoba irekhodi lomtapo liwanikeza. Akukona ukuhlolwa okugcwele kwengozi, ngakho funda ishidi lemininingwane yokuphepha elivela kumphakeli wakho. Ngaphambi kokuthi uthinte noma yikuphi okokwakha kwe-glaze, funda Ukuxuba ngokuphepha nomoya ohlanzekile futhi Ungawadliseli ushevu umndeni wakho.

Kusebenzise eresiphini

Engeza i-Jingdezhen Porcelain Stone, Sanbaopeng eresiphini ku-calculator ye-Glazecalc ukuze ubone ukuthi yenzani ku-unity formula ye-glaze.

Vula i-calculator yeresiphiKonke okokwakha okujwayelekile

Vula i-akhawunti yamahhala