Jingdezhen Porcelain Stone, Sanbaopeng
Malighafi ya kawaida katika maktaba ya Glazecalc: uchambuzi wake wa oksidi, mchango wake kwa UMF na hatari zake.
Ni nini
- Aina
- Feldspar na mawe
- Hali
- Ya kihistoria
- Fomula
- SiO₂ 73.7%, Al₂O₃ 15.34%, CaO 0.7%, MgO 0.16%, K₂O 4.13%, Na₂O 3.79%, Fe₂O₃ 0.7%, MnO 0.04%, LOI 1.13%
- Pia huitwa
- Sanbaopeng chinastone na San Bao porcelain stone
- Malighafi zinazofanana
- H&G Cornwall Stone , Cornish Stone (synthetic substitute) , Cornish Stone, Synthetic (Walker BA280) , Amakusa Pottery Stone (天草陶石)
- Chanzo
- He Z., Zhang M., Zhang H., 'Data-driven research on chemical features of Jingdezhen and Longquan celadon by energy dispersive X-ray fluorescence', arXiv:1511.07825 (2015), Table 6. Second analysis: derekau.net, 'Porcelain Stone Glazes' (2015), quoting 陶瓷艺术釉工艺学 (江西高校出版社) (2015)
Kihistoria: jiwe la porcelaini (瓷石) kutoka kijiji cha San Bao karibu na Jingdezhen, China, lililochimbwa huko na kuuzwa kwa viwanda vya ufinyanzi kama matofali; haliuzwi nje ya China. Huu ni uchambuzi mmoja, ambao makala inaunukuu kutoka kwa tafiti za awali za Kichina. Mwingine, kutoka kitabu cha glaze cha Jiangxi, ni karibu sawa, ukiwa na 17.64% Al₂O₃, 4.02% K₂O na 4.68% Na₂O, na jiwe kutoka San Bao hutofautiana kati ya wazalishaji na kutoka mwaka hadi mwaka.
Uchambuzi wa oksidi na fomula ya Seger
Glazecalc ina uchambuzi wa malighafi iitwayo Jingdezhen Porcelain Stone, Sanbaopeng kama asilimia ya uzito wa malighafi ghafi. Mchango kwa UMF ni moli za kila oksidi katika kiasi cha Jingdezhen Porcelain Stone, Sanbaopeng kinachobeba moli 1.0 ya flux, na hivyo ndivyo Glazecalc inavyoiongeza kwenye fomula ya Seger ya kichocheo.
| Oksidi | Uzito % | Mchango kwa UMF |
|---|---|---|
| SiO₂ | 73.7 | 10.053 |
| Al₂O₃ | 15.34 | 1.233 |
| CaO | 0.7 | 0.102 |
| MgO | 0.16 | 0.033 |
| K₂O | 4.13 | 0.359 |
| Na₂O | 3.79 | 0.501 |
| Fe₂O₃ | 0.7 | 0.036 |
| MnO | 0.04 | 0.005 |
- Uzito sawia
- 819.59
- Uzito baada ya kuchoma
- 810.33
- Upotevu wa uzito kwa moto
- 1.13%
Uzito sawia ni gramu za Jingdezhen Porcelain Stone, Sanbaopeng zinazobeba moli 1.0 ya flux. Uzito baada ya kuchoma ni kinachobaki kutoka kiasi hicho baada ya kuchoma.
Hatari na usalama
Hatari: Ina silika fuwele; epuka kuvuta vumbi lake.
Itumie katika kichocheo
Ongeza Jingdezhen Porcelain Stone, Sanbaopeng kwenye kichocheo katika kikokotoo cha Glazecalc ili kuona inavyobadilisha fomula ya Seger ya glaze.