Jingdezhen Porcelain Stone, Nangang
Kayan aiki na asali a laburaren Glazecalc: binciken oxide ɗinsa, gudummawar UMF da haɗarinsa.
Mene ne shi
- Nau’i
- Feldspar da duwatsu
- Matsayi
- Na tarihi
- Tsarin sinadarai
- SiO₂ 76.12%, Al₂O₃ 14.97%, CaO 1.45%, K₂O 2.77%, Na₂O 0.42%, Fe₂O₃ 0.76%, MnO 0.06%, LOI 3.71%
- Ana kuma kiransa
- Nangang chinastone
- Kayan aiki masu kama
- H&G Cornwall Stone , Cornish Stone (synthetic substitute) , Cornish Stone, Synthetic (Walker BA280) , Amakusa Pottery Stone (天草陶石)
- Tushe
- He Z., Zhang M., Zhang H., 'Data-driven research on chemical features of Jingdezhen and Longquan celadon by energy dispersive X-ray fluorescence', arXiv:1511.07825 (2015), Table 6 (2015)
Na tarihi: dutsen porcelain (瓷石) na masana'antun tukwane na Jingdezhen a China; ba a sayar da shi a wajen China. Wannan nazari ɗaya ne, wanda takardar ta ɗauko daga binciken China na baya; ba a ba da MgO da TiO₂ ba. Yadda aka haƙa shi aka shirya shi ba ya cikin majiyar.
Binciken oxide da UMF
Glazecalc yana da binciken Jingdezhen Porcelain Stone, Nangang a matsayin kashi bisa nauyi na ɗanyen kayan. Gudummawar UMF ita ce mole na kowane oxide a cikin adadin Jingdezhen Porcelain Stone, Nangang da ke ɗauke da mole 1.0 na flux, kuma haka Glazecalc ke ƙara shi cikin UMF (unity molecular formula) na tsarin glaze.
| Oxide | Kashi bisa nauyi % | Gudummawar UMF |
|---|---|---|
| SiO₂ | 76.12 | 20.146 |
| Al₂O₃ | 14.97 | 2.335 |
| CaO | 1.45 | 0.411 |
| K₂O | 2.77 | 0.468 |
| Na₂O | 0.42 | 0.108 |
| Fe₂O₃ | 0.76 | 0.076 |
| MnO | 0.06 | 0.013 |
- Nauyin daidai (equivalent weight)
- 1590.16
- Nauyi bayan gasa
- 1531.17
- LOI (raguwar nauyi a wuta)
- 3.71%
Nauyin daidai shi ne giram na Jingdezhen Porcelain Stone, Nangang da ke ɗauke da mole 1.0 na flux. Nauyi bayan gasa shi ne abin da ya rage daga wannan bayan gasa.
Haɗari da tsaro
Haɗari: Yana ƙunshe da crystalline silica; ku guji shaƙar ƙurar.
Yi amfani da shi a tsarin glaze
Ƙara Jingdezhen Porcelain Stone, Nangang cikin tsarin glaze a kalkuletan Glazecalc don ganin abin da yake yi wa UMF na glaze.