What it is

Kind
Feldspars and stones
Status
Historical
Formula
SiO₂ 76.12%, Al₂O₃ 14.97%, CaO 1.45%, K₂O 2.77%, Na₂O 0.42%, Fe₂O₃ 0.76%, MnO 0.06%, LOI 3.71%
Also called
Nangang chinastone
Similar materials
H&G Cornwall Stone , Cornish Stone (synthetic substitute) , Cornish Stone, Synthetic (Walker BA280) , Amakusa Pottery Stone (天草陶石)
Source
He Z., Zhang M., Zhang H., 'Data-driven research on chemical features of Jingdezhen and Longquan celadon by energy dispersive X-ray fluorescence', arXiv:1511.07825 (2015), Table 6 (2015)

Historical: a porcelain stone (瓷石) of the Jingdezhen potteries in China; it is not sold outside China. This is one analysis, which the paper quotes from earlier Chinese studies; MgO and TiO₂ were not given. How it was mined and prepared is not in the source.

Oxide analysis and unity formula

Glazecalc has the analysis of Jingdezhen Porcelain Stone, Nangang as weight percent of the raw material. The unity contribution is the moles of each oxide in the amount of Jingdezhen Porcelain Stone, Nangang that holds 1.0 mole of flux, which is how Glazecalc adds it into a recipe's unity formula.

Oxides in Jingdezhen Porcelain Stone, Nangang
Oxide Weight % Unity contribution
SiO₂76.1220.146
Al₂O₃14.972.335
CaO1.450.411
K₂O2.770.468
Na₂O0.420.108
Fe₂O₃0.760.076
MnO0.060.013
Equivalent weight
1590.16
Fired weight
1531.17
Loss on ignition
3.71%

The equivalent weight is the grams of Jingdezhen Porcelain Stone, Nangang that hold 1.0 mole of flux. The fired weight is what is left of that after firing.

Hazards and safety

Hazards: Contains crystalline silica; avoid breathing the dust.

Glazecalc shows the hazard wording as its record gives it. It is not a full risk assessment, so read the safety data sheet from your supplier. Before you handle any glaze material, read Safe mixing and ventilation and Don't poison your family.

Use it in a recipe

Add Jingdezhen Porcelain Stone, Nangang to a recipe in the Glazecalc calculator to see what it does to a glaze's unity formula.

Open the recipe calculatorAll standard materials

Create a free account