Kuyini

Uhlobo
Ama-feldspar namatshe
Isimo
Okomlando
I-formula
SiO₂ 76.12%, Al₂O₃ 14.97%, CaO 1.45%, K₂O 2.77%, Na₂O 0.42%, Fe₂O₃ 0.76%, MnO 0.06%, LOI 3.71%
Kubizwa nangokuthi
Nangang chinastone
Okokwakha okufanayo
H&G Cornwall Stone , Cornish Stone (synthetic substitute) , Cornish Stone, Synthetic (Walker BA280) , Amakusa Pottery Stone (天草陶石)
Umthombo
He Z., Zhang M., Zhang H., 'Data-driven research on chemical features of Jingdezhen and Longquan celadon by energy dispersive X-ray fluorescence', arXiv:1511.07825 (2015), Table 6 (2015)

Okomlando: itshe le-porcelain (瓷石) lezindawo zokubumba zase-Jingdezhen eShayina; alithengiswa ngaphandle kweShayina. Lokhu ukuhlaziywa okukodwa, okucashunwa yiphepha ezifundweni zangaphambili zaseShayina; i-MgO ne-TiO₂ azinikezwanga. Ukuthi lamajwa futhi lalungiswa kanjani akukho emthonjeni.

Ukuhlaziywa kwe-oxide ne-unity formula

I-Glazecalc inokuhlaziywa kwe-Jingdezhen Porcelain Stone, Nangang njengephesenti lesisindo sokokwakha okuluhlaza. Isabelo se-unity singama-mole e-oxide ngayinye enanini le-Jingdezhen Porcelain Stone, Nangang eliqukethe i-mole engu-1.0 ye-flux, okuyindlela i-Glazecalc eyengeza ngayo ku-unity formula yeresiphi.

Ama-oxide aku-Jingdezhen Porcelain Stone, Nangang
I-oxide Isisindo % Isabelo se-unity
SiO₂76.1220.146
Al₂O₃14.972.335
CaO1.450.411
K₂O2.770.468
Na₂O0.420.108
Fe₂O₃0.760.076
MnO0.060.013
Isisindo esilinganayo
1590.16
Isisindo esishisiwe
1531.17
I-loss on ignition
3.71%

Isisindo esilinganayo singamagremu e-Jingdezhen Porcelain Stone, Nangang aqukethe i-mole engu-1.0 ye-flux. Isisindo esishisiwe yilokho okusalayo kulokho ngemva kokushisa.

Izingozi nokuphepha

Izingozi: Kuqukethe i-silica eyikristalu; gwema ukuhogela uthuli.

I-Glazecalc ibonisa amagama engozi njengoba irekhodi lomtapo liwanikeza. Akukona ukuhlolwa okugcwele kwengozi, ngakho funda ishidi lemininingwane yokuphepha elivela kumphakeli wakho. Ngaphambi kokuthi uthinte noma yikuphi okokwakha kwe-glaze, funda Ukuxuba ngokuphepha nomoya ohlanzekile futhi Ungawadliseli ushevu umndeni wakho.

Kusebenzise eresiphini

Engeza i-Jingdezhen Porcelain Stone, Nangang eresiphini ku-calculator ye-Glazecalc ukuze ubone ukuthi yenzani ku-unity formula ye-glaze.

Vula i-calculator yeresiphiKonke okokwakha okujwayelekile

Vula i-akhawunti yamahhala