Waxa uu yahay

Nooca
Feldspar iyo dhagxaan
Xaaladda
Taariikhi
Qaacidada
SiO₂ 76.12%, Al₂O₃ 14.97%, CaO 1.45%, K₂O 2.77%, Na₂O 0.42%, Fe₂O₃ 0.76%, MnO 0.06%, LOI 3.71%
Sidoo kale loo yaqaan
Nangang chinastone
Walxo la mid ah
H&G Cornwall Stone , Cornish Stone (synthetic substitute) , Cornish Stone, Synthetic (Walker BA280) , Amakusa Pottery Stone (天草陶石)
Isha
He Z., Zhang M., Zhang H., 'Data-driven research on chemical features of Jingdezhen and Longquan celadon by energy dispersive X-ray fluorescence', arXiv:1511.07825 (2015), Table 6 (2015)

Taariikhi: dhagax porcelain (瓷石) oo ah kan warshadaha dhoobada Jingdezhen ee Shiinaha; lagama iibiyo Shiinaha dibaddiisa. Kani waa hal falanqayn, oo warqaddu ka soo xigatay daraasado Shiinees ah oo hore; MgO iyo TiO₂ lama bixin. Sida loo qoday loona diyaariyey kuma jiro isha.

Falanqaynta oksaydhka iyo UMF (unity molecular formula)

Glazecalc wuxuu hayaa falanqaynta walaxda Jingdezhen Porcelain Stone, Nangang oo ah boqolkiiba miisaanka walaxda ceeriin. Qaybta UMF waa moles-ka oksaydh kasta ee ku jira xaddiga walaxda Jingdezhen Porcelain Stone, Nangang ee haysta 1.0 mole oo flux ah, taasina waa sida Glazecalc ugu daro UMF-ta habka.

Oksaydhyada ku jira walaxda Jingdezhen Porcelain Stone, Nangang
Oksaydh Miisaan % Qaybta UMF
SiO₂76.1220.146
Al₂O₃14.972.335
CaO1.450.411
K₂O2.770.468
Na₂O0.420.108
Fe₂O₃0.760.076
MnO0.060.013
Miisaanka u dhigma (equivalent weight)
1590.16
Miisaanka kaddib gubidda
1531.17
LOI (lumista gubidda)
3.71%

Miisaanka u dhigma waa garaamada walaxda Jingdezhen Porcelain Stone, Nangang ee haysta 1.0 mole oo flux ah. Miisaanka kaddib gubidda waa inta ka hadha kaddib gubidda.

Khataraha iyo badbaadada

Khataraha: Waxaa ku jira silica kiristaal ah; iska ilaali neefsashada boodhka.

Glazecalc wuxuu muujiyaa qoraalka khatarta sida diiwaanka maktabaddu u bixiyo. Ma aha qiimayn khatar oo dhammaystiran, sidaas darteed akhri warqadda xogta badbaadada (SDS) ee alaab-qeybiyahaaga. Ka hor intaadan taaban walax glaze kasta, akhri Isku-darka ammaanka ah iyo hawo-wareejinta iyo Ha sumayn qoyskaaga.

Ku isticmaal hab

Ku dar walaxda Jingdezhen Porcelain Stone, Nangang hab ku jira xisaabiyaha Glazecalc si aad u aragto waxa ay ku samayso UMF-ta glaze-ka.

Fur xisaabiyaha habkaDhammaan walxaha caadiga ah

Samee akoon bilaash ah