What it is

Kind
Silica
Formula
SiO₂
Also called
Silica 200#, Silica 200 mesh (AU), Silica 200WQ, Silica Flour 200G, Walker BA770
Made by
Sibelco Australia (formerly Unimin Australia), Lang Lang, Victoria, Australia
Sold in
AU
Similar materials
Silica , Flint
Source
Unimin Australia, Technical Data - Silica 200WQ (Lang Lang), as posted by Clayworks Australia (archived)

Milled quartz flour (about 90% finer than 45 microns) from Sibelco's Lang Lang operation; the 'Silica 200#' sold by Walker (BA770), Keane, Northcote and Blackwattle. Walker's SDS names the Sibelco WQ series.

Oxide analysis and unity formula

Glazecalc has the analysis of Silica 200 Mesh (Sibelco Australia, Lang Lang) as weight percent of the raw material. The unity contribution is the moles of each oxide in the amount of Silica 200 Mesh (Sibelco Australia, Lang Lang) that holds 1.0 mole of flux, which is how Glazecalc adds it into a recipe's unity formula.

Silica 200 Mesh (Sibelco Australia, Lang Lang) has no flux oxide, so its unity contribution is per formula as written.

Oxides in Silica 200 Mesh (Sibelco Australia, Lang Lang)
Oxide Weight % Unity contribution
SiO₂99.31.653
Al₂O₃0.250.002
Fe₂O₃0.070.000
TiO₂0.010.000
Equivalent weight
100
Fired weight
99.7
Loss on ignition
0.3%

The equivalent weight is the grams of Silica 200 Mesh (Sibelco Australia, Lang Lang) that hold 1.0 mole of flux. The fired weight is what is left of that after firing.

Hazards and safety

Hazards: Sibelco SDS (milled silica products, 2011): quartz 99%, more than 20% respirable crystalline silica. Prolonged inhalation causes silicosis and lung cancer; avoid breathing the dust.

Glazecalc shows the hazard wording as its record gives it. It is not a full risk assessment, so read the safety data sheet from your supplier. Before you handle any glaze material, read Safe mixing and ventilation and Glaze safety at home.

Use it in a recipe

Add Silica 200 Mesh (Sibelco Australia, Lang Lang) to a recipe in the Glazecalc calculator to see what it does to a glaze's unity formula.

Open the recipe calculatorAll standard materials