What it is

Kind
Fluxes
Status
Historical
Formula
PbO
Similar materials
Lead Bisilicate Frit (Potclays 2261) , Lead Sesquisilicate Frit (Potclays 2262)
Source
Theoretical formula

Toxic heavy metal. Serious hazard from dust, can leach into solutions. Trace amounts can cause behavior changes in children and hamper learning.

Oxide analysis and unity formula

Glazecalc has the analysis of Lead, Yellow as moles of each fired oxide per formula. The unity contribution is the moles of each oxide in the amount of Lead, Yellow that holds 1.0 mole of flux, which is how Glazecalc adds it into a recipe's unity formula.

Oxides in Lead, Yellow
Oxide Moles Unity contribution
PbO11.000
Equivalent weight
223.2
Fired weight
223.2
Loss on ignition
0%

The equivalent weight is the grams of Lead, Yellow that hold 1.0 mole of flux. The fired weight is what is left of that after firing.

Hazards and safety

This material contains lead oxide (PbO).

Hazards: Danger (Carl Roth SDS, lead(II) oxide): H302+H332 harmful if swallowed or inhaled; H351 suspected of causing cancer; H360Df may damage the unborn child; H362 may harm breast-fed children; H372 damages kidneys, nervous system and blood-forming system; H410 very toxic to aquatic life.

Glazecalc shows the hazard wording as its record gives it. It is not a full risk assessment, so read the safety data sheet from your supplier. Before you handle any glaze material, read Safe mixing and ventilation and Glaze safety at home.

Use it in a recipe

Add Lead, Yellow to a recipe in the Glazecalc calculator to see what it does to a glaze's unity formula.

Open the recipe calculatorAll standard materials