What it is

Kind
Frits
Formula
SiO₂ 48.35%, B₂O₃ 22.62%, Na₂O 5.69%, CaO 11.36%, Al₂O₃ 11.98%
Also called
Frit 3195-2, F3195, Potclays 2274, Vibrantz Frit 3195, Frit 3195, Potterycrafts P3195 High Boro-Silicate Ferro Frit, CTM 111 Ferro Frit 3195, Vibrantz (Ferro) Frit 3195 (UK)
Made by
Vibrantz Technologies (formerly Ferro Corporation)
Sold in
US, UK, EU, AU
Similar materials
Fusion Frit F-2
Source
Ferro Corporation, 'USA Pottery Frits - Leadless Glaze Frits - Percentage Compositions', Version 11/08 (copy hosted by Digitalfire) (2008-11)

Well-balanced high-boron calcium borosilicate frit; about 85 frit to 15 kaolin makes a clear cone 04 glaze. Fusion 1500 F, flow 1700 F, CTE 7.16 (Ferro 2008).

Oxide analysis and unity formula

Glazecalc has the analysis of Ferro Frit 3195 as weight percent of the raw material. The unity contribution is the moles of each oxide in the amount of Ferro Frit 3195 that holds 1.0 mole of flux, which is how Glazecalc adds it into a recipe's unity formula.

Oxides in Ferro Frit 3195
Oxide Weight % Unity contribution
SiO₂48.352.734
B₂O₃22.621.104
Na₂O5.690.312
CaO11.360.688
Al₂O₃11.980.399
Equivalent weight
339.69
Fired weight
339.69
Loss on ignition
0%

The equivalent weight is the grams of Ferro Frit 3195 that hold 1.0 mole of flux. The fired weight is what is left of that after firing.

Hazards and safety

Hazards: Non-hazardous glass powder per supplier SDS; avoid breathing dust.

Glazecalc shows the hazard wording as its record gives it. It is not a full risk assessment, so read the safety data sheet from your supplier. Before you handle any glaze material, read Safe mixing and ventilation and Glaze safety at home.

Use it in a recipe