Chestnut Wood Ash, washed (栗灰)
Ihe a na-ejikarị n'ọbá akwụkwọ Glazecalc: nyocha oxide ya, ntinye unity ya na ihe ize ndụ ya.
Ihe ọ bụ
- Ụdị
- Flux
- Ọnọdụ
- Nke oge gara aga
- Formula
- K₂O 0.4%, MgO 5.6%, CaO 46.9%, Al₂O₃ 2%, SiO₂ 3.9%, P₂O₅ 3.4%, Fe₂O₃ 0.5%, LOI 36.4%
- A na-akpọkwa ya
- 栗灰, Chestnut ash, kuribai
- Ihe ndị yiri ya
- Synthetic Wood Ash (合成土灰)
- Ebe o si
- 吉田博和・児玉弘人・郡司恋緒菜・根本達志・新島佐知子「笠間長石と栗剪定枝焼却灰を用いた釉薬に関する研究」, 茨城県産業技術イノベーションセンター研究報告 53 (2024), 表1, 栗灰 E (2024)
Akụkọ ihe mere eme, ntụ obodo: alaka osisi chestnut a kpachara akpacha a gbara ọkụ na Kasama, Ibaraki, emesịa sachaa ya site n'itinye ya na mmiri na ịgbanwe mmiri ahụ oge ọ bụla o dosiri. Nke a bụ otu n'ime nlele isii (nlele E, nyocha XRF ọkara ọnụ ọgụgụ). N'ime isii ahụ, CaO sitere na 38.6% ruo 47.1% na SiO₂ sitere na 3.4% ruo 9.9%, silica ndị ọzọ sitere n'ala a kpọkọtara ya na ntụ ahụ. A naghị ere ya.
Nyocha oxide na unity formula
Glazecalc nwere nyocha Chestnut Wood Ash, washed (栗灰) dịka pasent ịdị arọ nke ihe ahụ a na-agbabeghị ọkụ. Ntinye unity bụ moles nke oxide ọ bụla n'ọnụ ọgụgụ Chestnut Wood Ash, washed (栗灰) nke nwere 1.0 mole nke flux; otu a ka Glazecalc si agbakwunye ya n'unity formula nke usoro.
| Oxide | Ịdị arọ % | Ntinye unity |
|---|---|---|
| K₂O | 0.4 | 0.004 |
| MgO | 5.6 | 0.142 |
| CaO | 46.9 | 0.854 |
| Al₂O₃ | 2 | 0.020 |
| SiO₂ | 3.9 | 0.066 |
| P₂O₅ | 3.4 | 0.024 |
| Fe₂O₃ | 0.5 | 0.003 |
- Ịdị arọ nhata (equivalent weight)
- 102.09
- Ịdị arọ mgbe a gbara ọkụ
- 64.93
- Loss on ignition (LOI)
- 36.4%
Ịdị arọ nhata bụ grams nke Chestnut Wood Ash, washed (栗灰) nke nwere 1.0 mole nke flux. Ịdị arọ mgbe a gbara ọkụ bụ ihe fọdụrụ na ya mgbe a gbachara ọkụ.
Ihe ize ndụ na nchekwa
Ihe ize ndụ: Ntụ osisi na-ere akpụkpọ ahụ (caustic), otu ahụkwa ka mmiri a na-eji asa ya dị: yiri uwe aka na ihe nchebe anya, ma zere iku uzuzu ahụ ume.
Jiri ya n'usoro
Tinye Chestnut Wood Ash, washed (栗灰) n'usoro na Glazecalc calculator ka ị hụ ihe ọ na-eme unity formula nke glaze.