What it is

Kind
Frits
Formula
SiO₂ 50.4%, B₂O₃ 25.2%, MgO 0.1%, Al₂O₃ 7.3%, Na₂O 12.1%, K₂O 3.4%, CaO 0.2%
Also called
Standard Alkaline Frit, Potterycrafts P2961
Sold in
UK
Source
Potterycrafts 'Standard Alkaline Frit' product page

Sodium borosilicate frit with about 25% B2O3 and almost no lime, recommended for copper turquoise glazes. Expansion 6.9 x 10^-6/°C, firing range 900-1100 °C.

Oxide analysis and unity formula

Glazecalc has the analysis of Standard Alkaline Frit (Potterycrafts P2961) as weight percent of the raw material. The unity contribution is the moles of each oxide in the amount of Standard Alkaline Frit (Potterycrafts P2961) that holds 1.0 mole of flux, which is how Glazecalc adds it into a recipe's unity formula.

Oxides in Standard Alkaline Frit (Potterycrafts P2961)
Oxide Weight % Unity contribution
SiO₂50.43.534
B₂O₃25.21.525
MgO0.10.010
Al₂O₃7.30.302
Na₂O12.10.822
K₂O3.40.152
CaO0.20.015
Equivalent weight
421.28
Fired weight
421.28
Loss on ignition
0%

The equivalent weight is the grams of Standard Alkaline Frit (Potterycrafts P2961) that hold 1.0 mole of flux. The fired weight is what is left of that after firing.

Hazards and safety

Hazards: Not classified (Potterycrafts SDS P2961); breathing the dust over long periods raises the risk of lung disease.

Glazecalc shows the hazard wording as its record gives it. It is not a full risk assessment, so read the safety data sheet from your supplier. Before you handle any glaze material, read Safe mixing and ventilation and Glaze safety at home.

Use it in a recipe

Add Standard Alkaline Frit (Potterycrafts P2961) to a recipe in the Glazecalc calculator to see what it does to a glaze's unity formula.