What it is

Kind
Colorants
Status
Historical
Formula
K₂Cr₂O₇
Also called
Potassium dichromate
Similar materials
Chromium Oxide
Source
Theoretical formula

Toxic. Chromium is counted as Cr₂O₃; the LOI is the oxygen released as it decomposes.

Oxide analysis and unity formula

Glazecalc has the analysis of Potassium Bichromate as moles of each fired oxide per formula. The unity contribution is the moles of each oxide in the amount of Potassium Bichromate that holds 1.0 mole of flux, which is how Glazecalc adds it into a recipe's unity formula.

Oxides in Potassium Bichromate
Oxide Moles Unity contribution
K₂O11.000
Cr₂O₃11.000
Equivalent weight
294.2
Fired weight
246.18
Loss on ignition
16.32%

The equivalent weight is the grams of Potassium Bichromate that hold 1.0 mole of flux. The fired weight is what is left of that after firing.

Hazards and safety

Hazards: Danger (Fisher UK SDS): H272 oxidiser; H301 toxic if swallowed; H312 harmful in contact with skin; H330 fatal if inhaled; H314 causes severe burns; H317/H334 skin and respiratory sensitiser; H340 may cause genetic defects; H350 may cause cancer; H360FD may damage fertility or the unborn child; H372 causes organ damage; H410 very toxic to aquatic life.

Glazecalc shows the hazard wording as its record gives it. It is not a full risk assessment, so read the safety data sheet from your supplier. Before you handle any glaze material, read Safe mixing and ventilation and Glaze safety at home.

Use it in a recipe

Add Potassium Bichromate to a recipe in the Glazecalc calculator to see what it does to a glaze's unity formula.

Open the recipe calculatorAll standard materials