What it is

Kind
Feldspars and stones
Formula
K₂O: 0.25; Na₂O: 0.75; Al₂O₃: 1.11; SiO₂: 4.65
Similar materials
Nepheline Syenite A270
Source
Glazecalc’s original data (2017), from a ceramics reference book

Typical formula. Higher ratio of fluxes makes this material melt at lower temps than most feldspars.

Oxide analysis and unity formula

Glazecalc has the analysis of Nepheline Syenite as moles of each fired oxide per formula. The unity contribution is the moles of each oxide in the amount of Nepheline Syenite that holds 1.0 mole of flux, which is how Glazecalc adds it into a recipe's unity formula.

Oxides in Nepheline Syenite
Oxide Moles Unity contribution
K₂O0.250.250
Na₂O0.750.750
Al₂O₃1.111.110
SiO₂4.654.650
Equivalent weight
462.6
Fired weight
462.6
Loss on ignition
0%

The equivalent weight is the grams of Nepheline Syenite that hold 1.0 mole of flux. The fired weight is what is left of that after firing.

Hazards and safety

Hazards: Not classified (Sibelco SDS, GB/IE); avoid breathing the dust.

Glazecalc shows the hazard wording as its record gives it. It is not a full risk assessment, so read the safety data sheet from your supplier. Before you handle any glaze material, read Safe mixing and ventilation and Glaze safety at home.

Use it in a recipe

Add Nepheline Syenite to a recipe in the Glazecalc calculator to see what it does to a glaze's unity formula.

Open the recipe calculatorAll standard materials