What it is

Kind
Fluxes
Formula
MgCO₃
Similar materials
Light Magnesium Carbonate
Source
Theoretical formula

MgCO₃, the mineral magnesite. Slightly soluble. Potters usually buy light magnesium carbonate, which has less MgO: see Light Magnesium Carbonate.

Oxide analysis and unity formula

Glazecalc has the analysis of Magnesium Carbonate (magnesite) as moles of each fired oxide per formula. The unity contribution is the moles of each oxide in the amount of Magnesium Carbonate (magnesite) that holds 1.0 mole of flux, which is how Glazecalc adds it into a recipe's unity formula.

Oxides in Magnesium Carbonate (magnesite)
Oxide Moles Unity contribution
MgO11.000
Equivalent weight
84.32
Fired weight
40.3
Loss on ignition
52.2%

The equivalent weight is the grams of Magnesium Carbonate (magnesite) that hold 1.0 mole of flux. The fired weight is what is left of that after firing.

Hazards and safety

Hazards: Not classified (CTM SDS 58); less than 1% quartz; avoid breathing the dust.

Glazecalc shows the hazard wording as its record gives it. It is not a full risk assessment, so read the safety data sheet from your supplier. Before you handle any glaze material, read Safe mixing and ventilation and Glaze safety at home.

Use it in a recipe

Add Magnesium Carbonate (magnesite) to a recipe in the Glazecalc calculator to see what it does to a glaze's unity formula.

Open the recipe calculatorAll standard materials