What it is

Kind
Feldspars and stones
Formula
SiO₂ 69.7%, Al₂O₃ 17.7%, Na₂O 6.9%, K₂O 4.3%, CaO 0.8%, Fe₂O₃ 0.08%, MgO 0.08%, TiO₂ 0.04%, LOI 0.4%
Also called
Feldspath mixte 64, Ceradel mixed feldspar 64
Sold in
EU
Similar materials
FFF Feldspar (Sibelco FFF K7-60)
Source
Ceradel product page 'Feldspath mixte 64'

A blend of feldspars with more soda (6.9%) than potash (4.3%), sold by Ceradel. It sits between a soda and a potash feldspar in melting behaviour.

Oxide analysis and unity formula

Glazecalc has the analysis of Feldspath mixte 64 (Ceradel) as weight percent of the raw material. The unity contribution is the moles of each oxide in the amount of Feldspath mixte 64 (Ceradel) that holds 1.0 mole of flux, which is how Glazecalc adds it into a recipe's unity formula.

Oxides in Feldspath mixte 64 (Ceradel)
Oxide Weight % Unity contribution
SiO₂69.76.697
Al₂O₃17.71.002
Na₂O6.90.643
K₂O4.30.264
CaO0.80.082
Fe₂O₃0.080.003
MgO0.080.011
TiO₂0.040.003
Equivalent weight
577.27
Fired weight
574.96
Loss on ignition
0.4%

The equivalent weight is the grams of Feldspath mixte 64 (Ceradel) that hold 1.0 mole of flux. The fired weight is what is left of that after firing.

Hazards and safety

Hazards: Fine dust contains respirable crystalline silica; avoid breathing it.

Glazecalc shows the hazard wording as its record gives it. It is not a full risk assessment, so read the safety data sheet from your supplier. Before you handle any glaze material, read Safe mixing and ventilation and Glaze safety at home.

Use it in a recipe

Add Feldspath mixte 64 (Ceradel) to a recipe in the Glazecalc calculator to see what it does to a glaze's unity formula.